Patents
US 8,758,528 B2#61609026 Most CitedActiveUnited States (USPTO)Utility

High-strength steel plate, method of producing the same, and high-strength steel pipe

1Forward Citations (#61609026 Global)
0.1/yrCitation Velocity (#49655423 Global)
0.75Citation PageRank (#61609026 Global)
16Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a high-strength steel plate having excellent resistance to cutting crack, excellent Charpy absorbed energy, excellent DWTT properties, a low yield ratio, and a tensile strength of 900 MPa or more, a method of producing the steel plate, and a high-strength steel pipe using the steel plate. As solving means, a steel plate contains, by % by mass, 0.03 to 0.12% of C, 0.01 to 0.5% of Si, 1.5 to 3% of Mn, 0.01 to 0.08% of Al, 0.01 to 0.08% of Nb, 0.005 to 0.025% of Ti, 0.001 to 0.01% of N, and at least one component of 0.01 to 2% of Cu, 0.01 to 3% of Ni, 0.01 to 1% of Cr, 0.01 to 1% of Mo, and 0.01 to 0.1% of V; wherein the contents of Ca, O, and S satisfy the equation below; the microstructure includes ferrite and a second hard phase, the area fraction of ferrite being 10 to 50%; cementite in the second phase has an average grin size of 0.5 μm or less; and the total amount of Nb and the like contained in carbides thereof present in steel is 10% or less of the total content in steel. 1≦(1−130×[O])×[Ca]/(1.25×[S])≦3 (1)

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A high-strength steel plate comprising a steel having the following components: by % by mass, 0.03 to 0.12% of C, 0.01 to 0.5% of Si, 1.5 to 3% of Mn, 0.01 to 0.08% of Al, 0.01 to 0.08% of Nb, 0.005 to 0.025% of Ti, 0.001 to 0.01% of N, 0.003% or less of O, 0.001% or less of S, and 0.0005 to 0.01% of Ca; and at least one component of 0.01 to 2% of Cu, 0.01 to 3% of Ni, 0.01 to 1% of Cr, 0.01 to 1% of Mo, and 0.01 to 0.1% of V; wherein the contents of Ca, O, and S satisfy the equation (1) below, and the balance is composed of Fe and inevitable impurities; 1≦(1−130×[O])×[Ca]/(1.25×[S])≦3 . . . (

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (16)

PatentTitleYearCitations
US 4,591,396 AMethod of producing steel having high strength and toughness198618
US 5,310,431 ACreep resistant, precipitation-dispersion-strengthened, martensitic stainless steel and method thereof199470
EP 0,733,715 A2Hot-rolled steel sheet and method for forming hot-rolled steel sheet having low yield ratio, high strength and excellent toughness—24
JP H08311548 AProduction of steel sheet for ultrahigh strength steel pipe excellent in toughness in weld zone—7
JP H09184012 AProduction of austenitic stainless steel sheet excellent in surface brightness characteristic abd corrosion resistance—2
JP H1017980 AWelded steel pipe with low yield ratio, and its production—15
JP H1017982 AHigh tensile strength steel material with low yield ratio for construction use, excellent in fracture resistance, and its production—36
US 5,755,895 AHigh strength line pipe steel having low yield ratio and excellent in low temperature toughness199861
JP H11302726 AProduction of high strength steel small in deviation of material—7
US 6,264,760 B1Ultra-high strength, weldable steels with excellent ultra-low temperature toughness200162
JP 2001335890 AHigh tensile steel sheet excellent in bendability, and its production method—28
JP 2003293089 AHigh strength steel sheet having excellent deformability, high strength steel pipe and production method thereof—38
WO 03,099,482 A1Uoe steel pipe with excellent crash resistance, and method of manufacturing the uoe steel pipe—6
EP 1,473,376 A1High strength steel plate and method for production thereof—14
US 2005178456 A1Uoe steel pipe with excellent crash resistance, and method of manufacturing the uoe steel pipe—12
US 6,958,099 B2High toughness steel material and method of producing steel pipes using same20058

Non-Patent Literature (1)

  • European Search Report for EP06731233 dated Jul. 7, 2011.