Patents
US 8,754,282 B2#31739466 Most CitedActiveUnited States (USPTO)Utility

Methods of consolidating radioactive containing materials by hot isostatic pressing

3Forward Citations (#31739466 Global)
0.2/yrCitation Velocity (#28725618 Global)
1.14Citation PageRank (#34920502 Global)
1Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present disclosure relates to a method of consolidating a calcine comprising radioactive material, the method comprising mixing 60-80% (by weight) of a radionuclide containing calcine with at least one non-radioactive additive, such as an oxide, and hot isostatic pressing the mixture to form a stable monolith of glass/ceramic. In one embodiment, the ratio of radionuclide containing calcine to additives is about 80:20 by weight, wherein the non-radioactive additive comprises oxides such as BaO, CaO, Al 2 O 3 , TiO 2 , SiO 2 and others, that combine with the waste elements and compounds to form a ceramic mineral or glass/ceramic material, after hot isostatic pressing. Non-limiting examples of mineral phases that may be formed are: hollandite (BaAl 2 Ti 6 O 16 ), zirconolite (CaZrThO 7 ), and perovskite (CaTiO 3 ).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of consolidating a calcined material comprising radioactive material, said method comprising: mixing a radionuclide containing calcine with at least one additive to form a pre-HIP powder; loading the pre-HIP powder into a can; sealing the can; loading the sealed can through a bottom of a HIP vessel; closing said HIP vessel; and hot-isostatic pressing the sealed can within the HIP vessel at a temperature ranging from 1000° C. to 1250° C. and a pressure ranging from 30 to 100 MPa for a time ranging from 10-14 hours.

  2. Claim 2Depends on #1

    The method of claim 1 , further comprising preheating the pre-HIP powder prior to loading it in the sealed can into the HIP vessel.

  3. Claim 3Depends on #2

    The method of claim 2 , wherein said preheating comprises heating the pre-HIP powder to a temperature sufficient to remove excess moisture fr

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (1)