Abstract

A method of using a catalyst comprises exposing a catalyst to at least one reactant in a chemical process. The catalyst comprises copper and a small pore molecular sieve having a maximum ring size of eight tetrahedral atoms. The chemical process undergoes at least one period of exposure to a reducing atmosphere. The catalyst has an initial activity and the catalyst has a final activity after the at least one period of exposure to the reducing atmosphere. The final activity is within 30% of the initial activity at a temperature between 200 and 500° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 4.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for using a catalyst comprising: a. exposing an SCR catalyst comprising copper and a small-pore molecular sieve having an AEI structure to a reducing atmosphere comprising NH 3 generated over a NO x adsorber catalyst and using the SCR catalyst to store NH 3 during the exposing step, and b. contacting the SCR catalyst with NO x in a non-reducing atmosphere to effect selective reduction of said NO x by the stored NH 3 .

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the small pore molecular sieve comprises SAPO-18 or SSZ-39.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein said silica-to-alumina ratio is from 8 to 150.