Tantalum sputtering target and method for manufacturing the same, and method for manufacturing semiconductor element
Abstract
In one embodiment, a method for manufacturing a tantalum sputtering target includes a first knead forging step, a first heating step, a second knead forging step, a cold rolling step, and a second heating step. In the first knead forging step, a tantalum material is subjected to two sets or more of knead forging, each of the sets being cold forging in directions parallel to and perpendicular to a thickness direction. In the second knead forging step, one set or more of knead forging is performed after the first heating step, each of the steps being cold forging in the directions parallel to and perpendicular to the thickness direction.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A tantalum sputtering target having a 99.99 wt % tantalum purity or more and a 50 μm average crystal grain size or less, wherein the tantalum sputtering target has a surface to be sputtered, and wherein, when X-ray diffraction (2θ) of the surface of the tantalum sputtering target is measured, peak relative intensities of (110), (211), and (200) planes become smaller in order of (110)>(211)>(200) which is equal to an intensity order of three major peaks in a Powder Diffraction File of tantalum.
- Claim 2Depends on #1
The tantalum sputtering target according to claim 1 , wherein a thickness is 10 mm or more.
- Claim 3Depends on #1
The tantalum sputtering target according to claim 1 , wherein, when X-ray diffraction (2θ) in a depth direction of the target is measured, peak relative intensities of (110), (211), and (200) planes become smalle