Patents
US 8,746,580 B2#22412941 Most CitedActiveUnited States (USPTO)Utility

Acousto-magnetic anti-theft label with a high coercivity bias and method of manufacture

5Forward Citations (#22412941 Global)
0.4/yrCitation Velocity (#19426440 Global)
1.13Citation PageRank (#35194921 Global)
15Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A high coercivity bias piece for making acousto-magnetic labels is made of an alloy strip with 10-14% weight percent Mn, less than 7% weight percent of one or more other transitional metals, with the balance Fe, after cold rolling to final gage, going through a final aging heat treatment at below 590 C, longer than 5 minutes. The strip thickness is 0.065-0.18 mm with coercivity measured by direct current method being 56-90 Oe. The method of making the high coercivity bias piece is to cold roll the strip to 0.07-0.15 mm with aging temperature at 450-570 C, for 0.5-20 hours to form a magnetic strip with coercivity of 60-85 Oe, followed by cutting the strip to required size. This high coercivity bias piece is manufactured without expensive Co and Ni materials, showing that a low cost Fe-(10-14% weight percent Mn) based alloy can be used to make high coercivity bias.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A bias piece for acousto-magnetic labels, comprising: an alloy strip having 10-14% by weight of Manganese, less than 7% by weight of one or more other transitional metals, and substantially balance Iron, cold rolled to final thickness of between 0.065-0.18 mm, with a final aging heat treatment at below 590 C for a period of time longer than 5 minutes to establish a coercivity measured by direct current method in the range of 56-90 Oe with a ratio of the residual magnetic flux density to the maximum magnetic flux density (Br/Bm) in the range of 65-88% where Bm is the magnetic induction at a max

  2. Claim 2Depends on #1

    The bias piece of claim 1 wherein the content of said one or more transitional metals is less than 5% by weight.

  3. Claim 3Depends on #1

    The bias piece of claim 1 w

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (15)

Non-Patent Literature (1)

  • Sungho Jin, "High-Remanence Square-Loop Fe-Ni and Fe-Mn Magnetic Alloys", IEEE Transactions on Magnetics vol. Mag-16 No. 5 Sep. 1980.