The present invention provides a method for manufacturing a cellulose nanofiber, characterized by comprising the step of fibrillating cellulose in a polyester based resin, preferably in a polyester based resin having an ester group concentration of 6.0 mmol/g or more and a cellulose nanofiber produced by the manufacturing method concerned. In addition, the present invention provides a masterbatch composition containing the cellulose nanofibers and the polyester based resin. Furthermore, the present invention provides a resin composition containing the masterbatch composition and a diluent resin and a processed product thereof.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 8.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a cellulose nanofiber comprising the step of fibrillating cellulose in a polyester based resin, wherein the ester group concentration of the polyester based resin is 6.0 mmol/g or more and the acid value is 10 KOHmg/g or more.

  2. Claim 2Independent Claim

    A method for manufacturing a cellulose nanofiber comprising the step of fibrillating cellulose in a polyester based resin, wherein the ester group concentration of the polyester based resin is 6.0 mmol/g or more and the hydroxyl value is 10 KOHmg/g or more.

  3. Claim 3Depends on #1, #2

    The method for manufacturing a cellulose nanofiber according to claim 1 or 2 , wherein the ester group concentration of the polyester based resin is 6.0 mmol/g or more, the acid value is 10 KOHmg/g or more, and the hydroxyl value is 10 KOHmg/g or more.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (14)

PatentTitleYearCitations
US 6,117,545 ASurface-modified cellulose microfibrils, method for making the same, and use thereof as a filler in composite materials200055
JP 2003165909 AWood-like resin composition stable in hue and molding using the same—12
JP 2005042283 AMethod for producing aliphatic polyester composition, pulp used for the same, and cellulosic fiber, and method for microfibrillating the same—70
JP 2005105081 AAliphatic polyester resin composition, its master batch and their films—4
JP 2006290972 AGelatinizing agent having highly dispersible cellulose composite and at least one polysaccharide—23
JP 2008242154 AFlexible substrate—24
JP 2009029927 AManufacturing method for thermoplastic resin composition, and manufacturing method for molded article—34
WO 2009/069641 A1Cellulose nanofiber and process for production thereof, and cellulose nanofiber dispersion—103
US 2009192264 A1Method of in situ bioproduction and composition of bacterial cellulose nanocomposites—39
JP 2009261993 AMethod of pulverizing polysaccharides, method of modifying polysaccharides, resin reinforcing agent and resin composition—31
WO 2010/050343 A1Solar battery rear surface protection sheet and solar battery module—5
JP 2010209510 AProcess for oxidation of cellulose and catalyst for oxidation of cellulose—14
US 2011263756 A1Molding material containing unsaturated polyester resin and microfibrillated plant fiber—33
US 8,420,735 B2Modified microfibrillated cellulose and resin composite material containing the same20135

Non-Patent Literature (2)

  • International Search Report dated Dec. 13, 2011, issued for PCT/JP2011/072070.
  • Machine Translation of JP 2005-042283, 2013.