US 8,735,294 B2#86099588 Most CitedActiveUnited States (USPTO)Utility

Method for fabricating a vertical LDMOS device

0Forward Citations (#86099588 Global)
0.0/yrCitation Velocity (#86099588 Global)
0.56Citation PageRank (#86099588 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A vertically arranged laterally diffused metal-oxide-semiconductor (LDMOS) device includes a trench extending into a semiconductor body toward a semiconductor substrate. The trench includes sidewalls, a bottom portion connecting the sidewalls, a dielectric material lining the trench and a diffusion agent layer lining the dielectric material. A lightly doped drain region adjoins the trench and extends laterally around the sidewalls from the diffusion agent layer into the semiconductor body. In one implementation, a method for fabricating a vertically arranged LDMOS device includes forming a trench extending into a semiconductor body toward a semiconductor substrate, the trench including sidewalls, a bottom portion connecting the sidewalls, a dielectric material lining the trench and a diffusion agent layer lining the dielectric material. The method further includes diffusing impurities from the diffusion agent layer through the dielectric material to form a lightly doped drain region extending laterally around the sidewalls into the semiconductor body.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating a vertically arranged laterally diffused metal-oxide-semiconductor (LDMOS) device comprising: forming a trench within a semiconductor body, said trench including sidewalls, a bottom portion, a dielectric material lining said trench and a diffusion agent layer lining said dielectric material; diffusing impurities from said diffusion agent layer through said dielectric material to form a lightly doped drain region extending laterally from said sidewalls of said trench into said semiconductor body.

  2. Claim 2Depends on #1

    The method for fabricating a vertically arranged LDMOS device of claim 1 , further comprising filling said trench with an insulative material.

  3. Claim 3Depends on #1

    The method for fabricating a vertically arranged LDMOS device of claim 1 , wherein said semiconductor body is of a first conductivity t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗