Patents
US 8,728,630 B2#71907297 Most CitedActiveUnited States (USPTO)Utility

Articles incorporating alloy deposits having controlled, varying nanostructure

0Forward Citations (#71907297 Global)
0.0/yrCitation Velocity (#71907297 Global)
0.56Citation PageRank (#71907297 Global)
24Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Bipolar wave current, is used to electrodeposit a nanocrystalline grain size. Polarity Ratio is the ratio of absolute value of time integrated amplitude of negative and positive polarity current. Grain size can be controlled in alloys of two or more components, at least one of which is a metal, and at least one of which is most electro-active. Typically, the more electro-active material is preferentially lessened during negative current. Current density, duration of pulse portions, and bath composition are determined with reference to relations showing grain size as a function of deposit composition, and deposit composition as a function of Polarity Ratio, or a single relation showing grain size as a function of Polarity ratio. A specified size can be achieved by selecting a corresponding Polarity Ratio. Coatings can be layered, each having an average grain size, which can vary layer to layer and also graded through a region.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An article of manufacture of a deposit comprising a nickel tungsten alloy or nickel molybdenum alloy, wherein the deposit comprises a coating on a substrate, the deposit comprising: a. a first layer region having a nanocrystalline structure with a first average grain size; b. adjacent said first layer region, and in contact therewith, a second layer region having a nanocrystalline structure with a second average grain size, which second size differs from the first size, wherein the difference between the first average grain size and the second average grain size is at least 50 nm; and further

  2. Claim 2Depends on #1

    The article of claim 1 , wherein the alloy comprises phosphorous.

  3. Claim 3Depends on #1

    The article of claim 1 , wherein the first layer region has a first nick

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 4,514,265 ABonding pads for semiconductor devices198529
US 4,652,348 AMethod for the production of alloys possessing high elastic modulus and improved magnetic properties by electrodeposition198749
JP S6431991 AManufacture of amorphous plating alloy—4
JP H02101192 AProduction of amorphous alloy—7
US 5,352,266 ANanocrystalline metals and process of producing the same1994141
US 5,433,797 ANanocrystalline metals1995172
US 5,489,488 ASoft magnetic film with compositional modulation and method of manufacturing the film199636
WO 9,918,266 A1Programmed pulse electroplating process—10
US 5,972,192 APulse electroplating copper or copper alloys1999304
US 6,036,833 AElectroplating method of forming platings of nickel200056
US 6,203,684 B1Pulse reverse electrodeposition for metallization and planarization of a semiconductor substrates200161
US 6,210,555 B1Electrodeposition of metals in small recesses for manufacture of high density interconnects using reverse pulse plating200167
US 6,319,384 B1Pulse reverse electrodeposition for metallization and planarization of semiconductor substrates200174
US 6,402,924 B1Programmed pulse electroplating process200231
JP 2002256478 AMETHOD FOR MANUFACTURING Cu-In LAMINATING FILM—7
JP 2003034891 AMethod for manufacturing cobalt iron alloy and plated magnetic thin-film of cobalt iron alloy, and method for manufacturing quaternary alloy and plated magnetic thin-film of cobalt iron molybdenum alloy—14
US 2003044303 A1Ultra high saturation moment soft magnetic thin film and its manufacturing method—24
JP 2003077723 ASoft magnetic film, method for manufacturing the same thin film magnetic head using the same and method for manufacturing the same—16
WO 2004/001100 A1Process for electroplating metallic and metall matrix composite foils, coatings and microcomponents—42
US 6,723,219 B2Method of direct electroplating on a low conductivity material, and electroplated metal deposited therewith200425
US 6,863,793 B2Sequential electrodeposition of metals using modulated electric fields for manufacture of circuit boards having features of different sizes200510
US 6,881,318 B2Dynamic pulse plating for high aspect ratio features200535
US 2005109626 A1Electrolytic process for depositing a graduated layer on a substrate, and component—13
US 2006046454 A1Method for filling electrically different features—11

Non-Patent Literature (5)

  • Abstract, Chemical Abstracts Service, Columbus, Ohio, US, 1987, Fei, Jingyin et al., "Electrodeposition of compositionally modulated zinc-cobalt alloy multilayer coatings", XP002554796, Chinese Journal of Chemical Engineering, 2005, 13(2), pp. 259-265.
  • Abstract, Chemical Abstracts Service, Columbus, Ohio, US, Apr. 2005, Ro, Boshin et al., "Pulse and periodic reverse current plating of palladium-nickel alloy", XP002554795, Nippon Kagaku Kaishi, 1987 (8), pp. 1593-9.
  • Chassaing, E., Roumegas, M.P., and Trichet, M.F., "Electrodeposition of Ni-Mo alloys with pulse reverse potentials", Journal of Applied Electrochemistry, (1995). 25(7): p. 667-70.
  • Cheung, C., Djuanda, F., Erb, U. and Palumbo, G, "Electrodeposition of nanocrystalline Ni-Fe alloys", Nanostructured Materials, vol. 5, No. 5, 1995, pp. 513-523.
  • Chinese Office Action dated Jun. 8, 2010 and English Translation thereof, from Chinese Pat. App. No. 200680028771.5, which is the Chinese National Phase of PCT/US2006/019830.