Poly(phenylene ether) fiber and method of making
Abstract
A fiber comprises a composition including a poly(phenylene ether) having less than or equal to 240 parts per million by weight of hydroxyl groups associated with ethylene bridge groups and less than or equal to 800 parts per million by weight of hydroxyl groups associated with rearranged backbone groups, both amounts based on the weight of the poly(phenylene ether). Fiber of low denier can be formed from this composition. The fiber can be formed by melt spinning.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A fiber comprising a composition comprising a poly(phenylene ether), wherein the fiber comprises hydroxyl groups associated with ethylene bridge groups and hydroxyl groups associated with rearranged backbone groups; and wherein the fiber comprises greater than 0 and less than or equal to 240 parts per million by weight of hydroxyl groups associated with ethylene bridge groups and greater than 0 to less than or equal to 800 parts per million by weight of hydroxyl groups associated with rearranged backbone groups, both amounts based on the weight of the poly(phenylene ether).
- Claim 2Depends on #1
The fiber of claim 1 , having a denier of less than or equal to 10.
- Claim 3Depends on #1
The fiber of claim 1 , wherein the composition comprises about 50 to 100 weight percent of the poly(phenylene ether), and 0 to about 50 weight percent of a
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Innovation Seminar; Microsoft PowerPoint Presentation; "Technical Textiles-High Performance Fibers"; Greensboro, NC; Oct. 13, 2005; 62 pages.
- International Search Report and Written Opinion; International Filing Date Dec. 13, 2012; Date of Mailing Apr. 8, 2013, P020427PCT; 9 pages.
- Liang, et al.; Elongation Properties of Polyethylene Melts; Polymer Engineering and Science; pp. 2490-2494; (2011).
- U.S. Appl. No. 13/229,066, filed Sep. 9, 2011, "Poly(arylene ether) Composition, Method, and Article".
- U.S. Appl. No. 14/132,672, filed with the USPTO on Dec. 18, 2013.