The application relates to a polyethylene composition having a base resin, the base resin comprising (A) a first polyethylene fraction, and (B) a second polyethylene fraction, wherein the melt flow rate MFR 5/190° c. of the first fraction is higher than the melt flow rate MFR 5/190° c. of the second fraction, the flow rate ratio FRR 21/5 of the polyethylene composition, defined as the ratio of melt flow rate MFR 21-6/190° c. to melt flow rate MFR 5/190° c. , is within the range of 15-28, and 10 the melt flow rate MFR 5/190° c. of the polyethylene composition is within the range of 0.5-1.1 g/10 min.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A multimodal polyethylene composition having a base resin, the base resin comprising (A) a first polyethylene fraction which is an ethylene homopolymer, and (B) a second polyethylene fraction, wherein the melt flow rate MFR 5/190° C. of the first fraction is higher than the melt flow rate MFR 5/190° C. of the second fraction; the flow rate ratio FRR 21/5 of the polyethylene composition, defined as the ratio of melt flow rate MFR 21.6/190° C. to melt flow rate MFR 5/190° C. , is within the range of 20-24; and the melt flow rate MFR 5/190° C. of the polyethylene composition is within the ra
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (13)
Non-Patent Literature (3)
- Equistar Technical Topic "Mold Shrinkage" (no date).
- International Search Report for International Application No. PCT/EP2005/011723.
- Viscosity Determination at 747 Pa Shear Stress filed in the European Opposition of EP 1,655,355 (2007).