Patents
US 8,720,563 B2#61141080 Most CitedActiveUnited States (USPTO)Utility

Calcium aluminate cement composition containing a set retarder of an organic acid and a polymeric mixture

1Forward Citations (#61141080 Global)
0.1/yrCitation Velocity (#49619074 Global)
0.75Citation PageRank (#61141080 Global)
29Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A cement composition for use in an oil or gas well, the cement composition comprises: a calcium aluminate cement; water; an organic acid; and a polymeric mixture comprising: (A) water; (B) citric acid; (C) a first polymer, wherein the first polymer: (i) comprises a cellulose backbone and carboxymethyl functional groups; and (ii) has a molecular weight of less than 100,000; and (D) a second polymer, wherein the second polymer: (i) comprises a lignosulfonate; and (ii) has a molecular weight of less than 100,000, wherein a test composition consisting essentially of: the cement; the water; the organic acid; and the polymeric mixture, and in the same proportions as in the cement composition has a thickening time of at least 5 hours at a temperature of 300° F. (148.9° C.) and a pressure of 10,000 psi (68.9 MPa).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of cementing in a subterranean formation comprising: introducing a cement composition into the subterranean formation, wherein the cement composition comprises: (A) a calcium aluminate cement; (B) water; (C) an organic acid; and (D) a polymeric mixture comprising: (i) water; (ii) citric acid; (iii) a first polymer, wherein the first polymer: (a) comprises a cellulose backbone and carboxymethyl functional groups; and (b) has a molecular weight of less than 100,000; and (iv) a second polymer, wherein the second polymer: (a) comprises a lignosulfonate; and (b) has a molecular weight of l

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (29)

PatentTitleYearCitations
US 5,447,197 AStorable liquid cementitious slurries for cementing oil and gas wells1995216
US 5,547,506 AStorable liquid cementitious slurries for cementing oil and gas wells1996160
JP 2,820,953 B2水中コンクリート組成物19982
US 6,143,069 ALight weight high temperature well cement compositions and methods200093
US 6,244,343 B1Cementing in deep water offshore wells200162
US 2001030044 A1Cementing in deep water offshore wells—4
US 6,332,921 B1Cement compositions and methods for high temperature wells containing carbon dioxide200195
US 6,488,763 B2Light weight high temperature well cement compositions and methods200262
US 6,708,760 B1Methods and cement compositions for cementing in subterranean zones200417
US 6,796,378 B2Methods of cementing high temperature wells and cement compositions therefor200431
US 6,835,243 B2Cementing in deep water offshore wells200418
US 6,846,357 B2Methods of cementing high temperature wells and cement compositions therefor200531
US 6,904,971 B2Cement compositions with improved corrosion resistance and methods of cementing in subterranean formations200529
US 7,008,479 B2Methods and cement compositions for cementing in subterranean zones20065
US 7,021,380 B2Compositions comprising set retarder compositions and associated methods200643
US 2006086502 A1Casing strings and methods of using such strings in subterranean cementing operations—34
US 7,285,165 B2Cement compositions comprising set retarder compositions and associated methods20077
US 7,337,842 B2Methods of using cement compositions comprising high alumina cement and cement kiln dust200821
US 7,381,263 B2Cement compositions comprising high alumina cement and cement kiln dust200826
US 7,390,356 B2Compositions for high temperature lightweight cementing200813
US 7,398,827 B2Methods for high temperature lightweight cementing200815
US 7,462,234 B2Wellbore servicing compositions20083
US 7,530,395 B2Methods of using wellbore servicing compositions20093
US 7,642,223 B2Methods of generating a gas in a plugging composition to improve its sealing ability in a downhole permeable zone201042
KR 20100040143 AEarly strength type concrete composition—6
US 7,748,454 B2Gelation inhibiting retarders for highly reactive calcium silicate based binder compositions and methods of making and using same20104
US 7,863,224 B2Wellbore servicing compositions comprising a set retarding agent and methods of making and using same201119
WO 2011/012922 A1Compositions and methods for servicing subterranean wells—3
US 2012073813 A1Novel Weight Materials for Use in Cement, Spacer and Drilling Fluids—39

Non-Patent Literature (5)

  • Brothers et al, Synthetic Retarder for High-Strength Cement, SPE/IADC, 21976, Mar. 1991, 659-665.
  • Dao et al, Environmentally Acceptable Cement Fluid Loss Additive, SPE, 74088, Mar. 2002, 1-6.
  • Dugonjic-Bilic et al, Study on Admixtures for Calcium Aluminate Phosphate Cement Useful to Seal CCS Wells, SPE, 141179, Apr. 2011, 1-12.
  • Reddy et al, Trends in the Development of Environmentally Acceptable Additives for Zonal Isolation Applications, SPE, 65393, Feb. 2001, 1-7.
  • Roshan, Characteristics of Oilwell Cement Slurry Using CMC, SPE, 114246, Sep. 2010, 328-335.