Abstract
According to an embodiment, a method for etching polycrystalline silicon includes a step of holding the polycrystalline silicon at a temperature higher than or equal to T E (K) given in a following equation; and a step of etching the polycrystalline silicon by dry etching with an etching gas containing CF 4 and O 2 , T E = - 0.114 x + 0.0556 k × ln { ( 1 - r / d ) × - 6.27 x + 5.38 - 2.01 x + 3.11 } where d (nm) is etching amount of the polycrystalline silicon, r (nm) is surface roughness of the polycrystalline silicon after the etching, x is ratio of flow rate of CF 4 gas to sum of flow rate of the CF 4 gas and flow rate of O 2 gas, and k (eV/K) is Boltzmann constant.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for etching polycrystalline silicon, comprising: holding the polycrystalline silicon at a temperature higher than or equal to T E (K) given in a following equation; and etching the polycrystalline silicon by dry etching with an etching gas containing CF 4 and O 2 , T E = - 0.114 x + 0.0556 k × ln {
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.