Tuning Tzc by the annealing of ultra low expansion glass
Abstract
The disclosure describes a method by which the Tzc of a silica-titania glass article, for example, a EUVL mirror substrate, can be tuned to within a specification range by means of a selected final anneal that shifts Tzc of the article or substrate to the desired Tzc value. In addition, since different mirrors in a set can be specified at different values of Tzc, this process can be on used glass samples or pieces from a single glass boule to make parts with different Tzc values, thus reducing the number of separate boules required to fill an order.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for adjusting the zero crossover temperature of a silica-titania glass, the method comprising the steps of: preparing a consolidated silica-titania glass boule having a titania content in the range of 5-20 wt %, annealing the consolidated silica-titania glass boule using a first anneal cycle to form a silica-titania glass having an initial state, the initial state including an initial zero crossover temperature Tzc 0 and an initial fictive temperature Tf 0 , determining the initial zero crossover temperature Tzc 0 and the initial fictive temperature Tf 0 of the silica-titania glass
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 10,427,974 B2 | Glass composite for use in extreme ultra violet lithography | 2019 | 4 |