Hydrothermal synthesis of nanocubes of sillenite type compounds for photovoltaic applications and solar energy conversion of carbon dioxide to fuels

3Forward Citations (#31509711 Global)
0.2/yrCitation Velocity (#28702126 Global)
1.15Citation PageRank (#34305585 Global)
1Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to formation of nanocubes of sillenite type compounds, such as bismuth titanate, i.e., Bi 12 TiO 20 , nanocubes, via a hydrothermal synthesis process, with the resulting compound(s) having multifunctional properties such as being useful in solar energy conversion, environmental remediation, and/or energy storage, for example. In one embodiment, a hydrothermal method is disclosed that transforms nanoparticles of TiO 2 to bismuth titanate, i.e., Bi 12 TiO 20 , nanocubes, optionally loaded with palladium nanoparticles. The method includes reacting titanium dioxide nanotubes with a bismuth salt in an acidic bath at a temperature sufficient and for a time sufficient to form bismuth titanate crystals, which are subsequently annealed to form bismuth titanate nanocubes. After annealing, the bismuth titanate nanocubes may be optionally loaded with nano-sized metal particles, e.g., nanosized palladium particles.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of making bismuth titanate nanocubes comprising: reacting titanium dioxide nanotubes with a bismuth salt in an acidic bath at a temperature sufficient and for a time sufficient to form bismuth titanate crystals having the formula Bi 12 TiO 20 , where Bi is bismuth; Ti is titanium or a fraction thereof between 0 and 1; and O is oxygen; and annealing the bismuth titanate crystals to form bismuth titanate nanocubes, wherein the acidic bath has a bismuth salt concentration of from about 0.1M to 3M.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the acidic bath has a pH of 0 to 2.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the temperature sufficient is from about 110° C. to about 175° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (1)

Non-Patent Literature (5)

  • Anpo et al., Photocatalytic reduction of CO2 with H2O on various titanium oxide catalysts, Journal of Electroanalytical Chemistry, 1995, pp. 21-26, vol. 396.
  • Chanmanee et al., Formation and Characterization of Self-Organized TiO2 Nanotube Arrays by Pulse Anodization, Journal of American Chemical Society, 2008, pp. 965-974, vol. 130.
  • Hinogami et al., An Approach to Ideal Smiconductor Electrodes for Efficient Photoelectrochemical Reduction of Carbon Dixoide by Modification with Small Metal Particles, Journal of Physical Chemistry B, 1998, pp. 974-980, vol. 102, No. 6.
  • Holt-Hindle et al., Electrocatalytic Activity of Nanoporous Pt-Ir Materials toward Methanol Oxidation and Oxygen Reduction, Journal of the Electrochemical Society, 2008, pp. K5-59, vol. 155, No. 1.
  • Indrakanti et al., Quantum Mechanical Modeling of CO2 Interactions with Irradiated Stoichiometric and Oxygen-Deficient Antase TiO2 Surfaces: Implications for the Photocatalytic Reduction of CO2, Energy & Fuels, Aug. 28, 2008, pp. 5247-5256, vol. 23.