US 8,709,124 B2#129382921 Most CitedActiveUnited States (USPTO)Utility

Sintered sliding member

0Forward Citations (#129382921 Global)
0.0/yrCitation Velocity (#129382921 Global)
0.56Citation PageRank (#129382921 Global)
10Prior Art Cited
3Claims (3 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

There is provided a novel sintered sliding member superior in thermal resistance, corrosion resistance and wear resistance. The sintered sliding member of the present invention includes 7.7-30.3% Cu, 2.0-20.0% Sn and 0.3-7.0% boron nitride by mass, with a remainder composed of Ni and unavoidable impurities. The sintered sliding member may further include 0.1-3.0% C or 0.1-0.7% P. A porosity of the sintered sliding member is 5-25%.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (3 — 3 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A sintered sliding member comprising, by mass %:

  2. Claim 2Independent Claim

    0-20.0% Sn; 0.3-7.0% boron nitride; 0.1-0.7% P; and a remainder including Ni and unavoidable impurities.

  3. Claim 3Independent Claim

    A sintered sliding member comprising, by mass %:

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • International Search Report mailed Feb. 8, 2011 for the corresponding International Application No. PCT/JP2010/071879.