High strength tape articles from ultra-high molecular weight polyethylene

0Forward Citations (#86373025 Global)
0.0/yrCitation Velocity (#86373025 Global)
0.56Citation PageRank (#86373025 Global)
35Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Tape articles having improved properties are made from ultra-high molecular weight (UHMW) multi-filament yarns. The tape articles can have a ratio of the low temperature area under the curve (120° C. to Tm-onset) to the total area under the curve (120° C. to 165° C.) of less than about 0.15 as calculated from an increasing temperature DSC scan from a temperature of 30° C. to a temperature of 200° C. at a constant rate of 10° C. per minute. Additionally, in some examples the tape articles can also have a tenacity at least about 24 g/d (2.06 GPa) when measured by ASTM D882-09 at a 10 inch (25.4 cm) gauge length and at an extension rate of 100%/min. Further, the tape articles can have no long period of less than 450 Angstroms (Å) when measured by small angle x-ray analysis.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A tape article made from ultra-high molecular weight polyethylene multi-filament yarn, the tape article comprising: an average cross-sectional aspect ratio of at least about 10:1; and a ratio of the low temperature area under the curve (120° C. to Tm-onset) to the total area under the curve (120° C. to 165° C.) of less than about 0.15 as measured by an increasing temperature DSC scan from a temperature of 30° C. to a temperature of 200° C. at a constant rate of 10° C. per minute.

  2. Claim 2Depends on #1

    The tape article of claim 1 , wherein the tape article has a tenacity of at least about 24 g/d (2.07 GPa) when measured by ASTM D882-09 at a 10 inch (25.4 cm) gauge length and at an extension rate of 100%/min, and wherein said average cross-sectional aspect ratio is at least about 50:1.

  3. Claim 3Depends on #2

    The tape article of claim 2 , wherein

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (35)

PatentTitleYearCitations
US 4,413,110 AHigh tenacity, high modulus polyethylene and polypropylene fibers and intermediates therefore1983646
US 4,623,574 ABallistic-resistant composite article1986320
US 4,748,064 ABallistic-resistant composite article1988183
US 4,819,458 AHeat shrunk fabrics provided from ultra-high tenacity and modulus fibers and methods for producing same198933
US 4,996,011 AProduction of polyethylene materials having improved strength and modulus qualities199145
US 5,091,133 AContinuous production process of high-strength and high-modulus polyolefin material1992100
US 5,106,555 AProcess for the continuous production of high-strength and high-modulus polyethylene material199274
US 5,135,804 ANetwork of polyethylene fibers199271
US 5,200,129 AProcess for continuous production of polyolefin material199366
US 5,540,990 APolyolefin line199642
US 5,578,373 ASplit polyethylene stretched material and process for producing the same1996117
US 5,628,946 AProcess for producing polymeric materials199747
US 5,749,214 ABraided or twisted line199847
US 6,017,834 AMonoliyhic polymeric product200023
US 6,148,597 AManufacture of polyolefin fishing line200077
US 6,328,923 B1Process of making a compacted polyolefin article200129
US 2002037391 A1Flexible fabric from fibrous web and discontinuous domain matrix—63
US 6,458,727 B1Olefin polymers200244
US 6,743,388 B2Process of making polymer articles200454
US 6,951,685 B1Ultra high molecular weight polyethylene fibers200575
EP 1,627,719 A1Multilayered polyethylene material and ballistic resistant articles manufactured therefrom—171
WO 2006/074823 A1Dental tape and process for its manufacturing—7
WO 2007/107359 A1Process for the manufacture of a shaped part and shaped part obtainable with said process—41
US 7,279,441 B2Compacted olefin fibers20079
US 7,311,963 B2Process for the production of a shaped article20078
US 2008064280 A1High performance ballistic composites having improved flexibility and method of making the same—25
US 7,407,900 B2Unique ballistic composition200815
US 2008251960 A1Multiple calender process for forming non-fibrous high modulus ultra high molecular weight polyethylene tape—39
US 2008318016 A1Non-fibrous high modulus ultra high molecular weight polyethylene tape for ballistic applications—27
US 7,470,459 B1Ultra high molecular weight polyethylene ballistic structures200815

Non-Patent Literature (5)

  • Akira Kaito et al., "Hot Rolling and Quench Rolling of Ultrahigh Molecular Weight Polyethylene," Journal of Applied Polymer Science, vol. 28, pp. 1207-1220, 1983.
  • Akira Kaito et al., "Preparation of High Modulus Polyethylene Sheet by the Roller-Drawing Method," Journal of Applied Polymer Science, vol. 30, pp. 1241-1255, 1985.
  • Akira Kaito et al., "Roller Drawing of Ultrahigh Molecular Weight Polyethylene," Journal of Applied Polymer Science, vol. 30, pp. 4591-4608, 1985.
  • Eunji Lee et al., "Rigid-flexible block molecules based on a laterally extended aromatic segment: Hierarchical assembly into single fibers, flat ribbons, and twisted ribbons," Chemistry-A European Journal, vol. 14, No. 23, pp. 6957-6966, Aug. 8, 2008.
  • Li-Hui Wang et al., "New approach for processing ultrahigh-molecular weight polyethylene powder. Solid-state rolling followed by hot stretch (roll-draw)," Journal of Polymer Science, Part B: Polymer Physics, vol. 28, No. 12, pp. 2441-2444, Nov. 1990 (Abstract only).