US 8,697,186 B2#65261499 Most CitedActiveUnited States (USPTO)Utility

Method for manufacturing a mask having submillimetric apertures for a submillimetric electrically conductive grid, and mask and submillimetric electrically conductive grid

0Forward Citations (#65261499 Global)
0.0/yrCitation Velocity (#65261499 Global)
0.56Citation PageRank (#65261499 Global)
20Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for manufacturing a mask having submillimetric openings, in which: for a masking layer, a first solution of colloidal nanoparticles in a first solvent is deposited, the particles having a given glass transition temperature T g , the drying of the masking layer, known as the first masking layer, is carried out at a temperature below said temperature T g until a mask having a two-dimensional network of substantially straight-edged submillimetric openings, that defines a mask zone known as a network mask zone is obtained, a solid mask zone is formed by a liquid deposition, on the face, of a second masking zone, the solid mask zone being adjacent to and in contact with the network mask zone, and/or at least one cover zone is formed, the cover zone being in contact with the network mask zone, and/or after the drying of the first masking layer, a filled mask zone is formed by filling, via a liquid route, openings of a portion of the network mask zone. The invention also relates to the mask and the electroconductive grid obtained.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for manufacturing a mask having submillimetric openings, the mask produced on a main face of a substrate by deposition of a liquid masking layer as a solution and drying, the process comprising: depositing a first solution of colloidal nanoparticles stabilized and dispersed in a first solvent to form a first masking layer, the nanoparticles having a glass transition temperature T g ; drying the first masking layer at a temperature below said temperature T g until a network mask having a two-dimensional network of submillimetric openings is obtained with substantially straight mask a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 4,435,047 AEncapsulated liquid crystal and method1984559
EP 0,238,164 A1Liquid crystal panel—49
US 4,732,456 AScattering display for contrast enhancement including target198854
US 4,806,922 ADisplay device utilizing a plurality of NCAP liquid crystal modules198944
WO 9,219,695 A2Crystalline light modulating device and material—62
US 5,453,459 ATemporary coating system199543
US 5,866,199 APrimer-paint mask composition and methods of use thereof199927
WO 0,050,354 A1Glass coating—14
WO 2004/015739 A2Flat lamp, production method thereof and application of same—12
US 2004150326 A1Network conductor and its production method and use—54
WO 2004/085135 A2Method of depositing functional films on substrates such as glass sheets and film-coating machine for implementing said method—8
US 2005059766 A1Durable optical element—91
EP 1,610,940 A2Method of depositing functional films on substrates such as glass sheets and film-coating machine for implementing said method—3
WO 2006/090086 A2Planar or substantially planar luminous structure—4
US 7,172,822 B2Network conductor and its production method and use200737
WO 2007/023237 A2Flat coplanar-discharge lamp and uses of same—8
WO 2007/042689 A2Flat uv lamp with coplanar discharge and uses thereof—2
WO 2008/023124 A1Substantially flat luminous and/or uv structure—3
WO 2008/132397 A2Process for fabricating a mask with submillimetre apertures for the production of a submillimetre grid, and submillimetre grid—12
FR 2,924,274 A1Substrat porteur d'une electrode, dispositif electroluminescent organique l'incorporant, et sa fabrication—12

Non-Patent Literature (3)

  • Adelung, et al., "Strain-controlled growth of nanowires within thin-film cracks", Nature Materials, Nature Publishing Group, vol. 3, Jun. 2004, pp. 375-379.
  • International Preliminary Report on Patentability, including the Written Opinion dated Feb. 18, 2010, as issued for PCT/FR2009/051816, dated May 31, 2011.
  • International Search Report as issued for PCT/FR2009/051816, dated Feb. 18, 2010.