Particulate mixture, active material aggregate, cathode active material, cathode, secondary battery and methods for producing the same

0Forward Citations (#62378086 Global)
0.0/yrCitation Velocity (#62378086 Global)
0.56Citation PageRank (#62378086 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A particulate mixture which can be used as a precursor of lithium transition metal silicate-type compound of small particle size and low crystallinity, is provided. It is a mixture of silicon oxide particulates, transition metal oxide particulates, and lithium transition metal silicate particulates, and its powder X-ray diffraction measurement shows diffraction peaks near 2θ=33.1° and near 2θ=35.7°, and said silicon oxide particulates and said transition metal oxide particulates are amorphous, and said lithium transition metal silicate particulates are in a microcrystalline or amorphous state.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A particulate mixture, which comprises silicon oxide particulates, transition metal oxide particulates, and lithium transition metal silicate particulates; wherein the powder X-ray diffraction measurement of the particulate mixture shows diffraction peaks near 2θ=33.1° and near 2θ=35.7°; said silicon oxide particulates and said transition metal oxide particulates are amorphous; and said lithium transition metal silicate particulates are in a microcrystalline or amorphous state.

  2. Claim 2Depends on #1

    The particulate mixture according to claim 1 , wherein the full width at half maximum of the diffraction peak near 2θ=33.1° is 0.35° or more, and wherein the full width at half maximum of the diffraction peak near 2θ=35.7° is 0.35° or more.

  3. Claim 3Depends on #1

    The particulate mixture according to claim 1 , wherein said transition metal o

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (2)

  • International Search Report for PCT/JP2011/054351 mailed May 17, 2011.
  • Miki Yasutomi et al. "Synthesis and Electrochecmical Properties of Li2-xM(SiO4)1-x(PO4)x(M = Fe, Mn) Positive Active Materials by Hydrothermal Process for Li-ion Cells" GS Yuasa Technical Report, GS Yuasa Corporation, Jun. 26, 2006, vol. 6, No. 1, pp. 21-26.