Compositions and methods for improving the toughness of set cements
Abstract
The toughness of set cement may be enhanced by incorporating partially cured waterborne resins in the cement matrix. A hardening agent is added to the waterborne resin, and the mixture is allowed to react for periods between about 1 min and 15 min. The waterborne resin with hardening agent is then combined with an inorganic cement to form a pumpable slurry.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 21.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for treating a subterranean well, comprising: (i) providing a first composition comprising a slurry comprising an inorganic cement and a retarder comprising a lignosulfonate, a hydrocarboxylic acid, or a phosphonate or a combination thereof; (ii) providing a second composition comprising a waterborne resin having an initial particle size; (iii) adding a hardening agent to the second composition, and allowing the hardening agent to react with the resin; (iv) mixing the first composition with the second composition containing the hardening agent; and (v) placing the resulting mixture in
- Claim 2Independent Claim
The method of claim
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 21 total)
References Cited — Backward Prior Art (23)
Non-Patent Literature (1)
- Nelson EB, Drochon B, Michaux M and Griffin TJ: "Special Cement Systems," in Nelson EB and Guillot D (eds): Well Cementing-2nd Edition, Schlumberger, Houston (2006) 233-268.