Magnetically insensitive, highly hard and constant-modulus alloy, and its production method, as well as hair spring, mechanical driving apparatus and watch and clock
Abstract
A constant-modulus alloy, which has a low saturation magnetic flux density to provide weakly magnetic properties, a high Young's modulus, a low temperature coefficient of Young's modulus, and high hardness, is provided. A hairspring, a mechanical driving apparatus and a watch and clock, in which the alloy is used, are provided. The alloy consists of Co, Ni, Cr, Mo. and Fe. The alloy is healed and cooled before being subjected to repeated wiredrawing and intermediate annealing, forming a wire with a fiber structure having a <111> fiber axis. The wire is then cold rolled into a sheet and heated to obtain optimal magnetic insensitivity and hardness.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 4.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A magnetically insensitive, highly hard, constant-modulus alloy, containing, by atomic weight ratio, 20-40% Co and 7 to 22% Ni, with the total of Co and Ni being 42.0 to 49.5%, 5 to 13% Cr and 1 to 6% Mo, with the total of Cr and Mo being 13.5 to 16.0%, and with the balance being essentially Fe (with the proviso that Fe is present 37% or more) and inevitable impurities, characterized in that the alloy has a {110}<111> texture, as well as a saturation magnetic flux density of 2500 to 3500 G, a temperature coefficient of Young's modulus of (−5˜+5)—10 −5 degrees C. −1 of as measured a
- Claim 2Depends on #1
A magnetically insensitive, highly hard, constant-modulus alloy according to claim 1 , further containing as an auxiliary element(s) 5% or less of one or more of W, V, Cu, M
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (4 of 4 total)
References Cited — Backward Prior Art (16)
Non-Patent Literature (5)
- Extended European Search Report dated Jan. 15, 2013, issued in corresponding European Patent Application No. 09 826 188.6.
- International Preliminary Report on Patentability (Form PCT/IB/373) of International Application No. PCT/JP2009/069458 mailed May 17, 2011 with Forms PCT/IB/326 and PCT/ISA/237.
- International Preliminary Report on Patentability dated Jun. 21, 2011, issued in corresponding International Application No. PCT/JP2009/069458.
- International Search Report of PCT/JP2009/069458, mailing date Feb. 16, 2010.
- Masumoto Hakaru et al; "On the Elastic Anisotropies and its Temperature Change of Single Crystals of High Elasticity Alloy "Dia-flex" in the Co-Fe-Ni-Cr-W-Mo System", Bulletin of Japan Institute Society for Meals (1967); pp. 263-268.