Patents
US 8,679,302 B2#61551556 Most CitedActiveUnited States (USPTO)Utility

Silicon titanium oxide coating, coated article including silicon titanium oxide coating, and method of making the same

1Forward Citations (#61551556 Global)
0.1/yrCitation Velocity (#49650879 Global)
0.75Citation PageRank (#61551556 Global)
19Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Certain example embodiments relate to a layer of or including Ti 1-x Si x O y and/or a method of making the same. In certain example embodiments, the Ti 1-x Si x O y -based layer may be substoichiometric with respect to oxygen. In certain example embodiments of this invention, the layer may include Ti 1-x Si x O y where x is from about 0.05 to 0.95 (more preferably from about 0.1 to 0.9, and even more preferably from about 0.2 to 0.8, and possibly from about 0.5 to 0.8) and y is from about 0.2 to 2 (more preferably from about 1 to 2, and even more preferably from about 1.5 to 2, and possibly from about 1.9 to 2). The layer may have an index of refraction of from about 1.6 to 1.9. The layer may also be used with a transparent conductive oxide in a transparent conductive coating.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for making a coated article, the method comprising: sputter-depositing a first medium index layer comprising Ti 1-x Si x O y on a glass substrate, where x is from 0.05 to 0.95 and y is from 0.2 to 2, wherein said medium index layer comprising Ti 1-x Si x O y , is sputter-deposited by a target comprising Si and Ti, wherein the ratio of Si to Ti in the target is from 3:1 to 2:1, forming a high index layer comprising an oxide of titanium over and contacting the medium index layer; and forming a low index layer comprising an oxide of silicon over and contacting the high index layer, wher

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
EP 0,331,201 A1Amorphous oxide film and article having such film thereon—29
US 5,110,637 AAmorphous oxide film and article having such film thereon1992130
EP 0,515,847 A2Glass pane with reflectance reducing coating—32
JP H05214526 ACeramic rotational cathode target and its manufacture—12
US 5,427,665 AProcess and apparatus for reactive coating of a substrate199553
JP H07233469 ATarget, its production and production of high-refractive-index film—57
US 5,470,452 AShielding for arc suppression in rotating magnetron sputtering systems199564
JP H08158048 ATarget and its production and formation of film high in refractive index—6
US 5,605,609 AMethod for forming low refractive index film comprising silicon dioxide199744
US 5,725,746 AShielding for arc suppression in rotating magnetron sputtering systems199863
EP 0,953,550 A1Low-reflectance glass article and process for preparating the same—17
US 6,309,753 B1Coated ultraviolet absorbing glass200123
EP 1,153,658 A1Visible light response type photocatalyst—6
EP 1,176,434 A1Substrate provide with antireflection films and its production method—9
US 6,743,343 B2Target and process for its production, and method of forming a film having a high refractive index200432
US 2004163943 A1Cylindrical magnetron with self cleaning target—17
WO 2007/013261 A1Sputtering target, method for producing same, sputtering thin film formed by using such sputtering target, and organic el device using such thin film—3
US 2007108043 A1Sputtering target including titanium silicon oxide and method of making coated article using the same—18
US 2010040892 A1Coated article with transparent conductive oxide film doped to adjust Fermi level, and method of making same—6

Non-Patent Literature (1)

  • U.S. Appl. No. 11/272,448, filed Nov. 14, 2005; Lu.