Patents
US 8,673,170 B2#12407608 Most CitedActiveUnited States (USPTO)Utility

Non-homogenous positive electrode materials combining high safety and high power in a Li rechargeable battery

8Forward Citations (#12407608 Global)
0.7/yrCitation Velocity (#11232427 Global)
4.19Citation PageRank (#4410606 Global)
12Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a Li a Ni x Co y M z O 2±e A f composite oxide for use as a cathode material in a rechargeable battery, with a non-homogenous Ni/Al ratio in the particles, allowing excellent power and safety properties when used as positive electrode material in Li battery. More particularly, in the formula 0.9<a<1.1, 0.3≦x≦0.9, 0≦y≦0.4, 0<z≦0.35, e=0, 0≦f≦0.05 and 0.9<(x+y+z+f)<1.1; M consists of either one or more elements from the group Al, Mg and Ti; A consists of either one or more elements from the group S and C. The powder has a particle size distribution defining a D10, D50 and D90; and said x and z parameters varying with the particles size of said powder, and is characterized in that either one or both of: x1−x2≧0.010 and z2−z1≧0.010; x1 and z1 being the parameters corresponding to particles having a particle size D90; and x2 and z2 being the parameters corresponding to particles having a particle size D10.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A lithium metal oxide powder for use as a cathode material in a rechargeable battery, having the general formula Li a Ni x Co y M z O 2±e A f , wherein 0.9<a<1.1, 0.3≦x≦0.9, 0<y≦0.4, 0<z≦0.35, e<0.02, 0≦f≦0.05 and 0.9<(x+y+z+f)<1.1; wherein M comprises one or more elements selected from the group consisting of Al, Mg, and Ti; A comprises either one or both of S and C; wherein said powder has a particle size distribution defining a D10, D50 and D90; and said x and z parameters vary with the particle size of said powder; wherein either one or both of: x1−x2≧0.010 and z2−z1≧0

  2. Claim 2Depends on #1

    The powder of claim 1 , whe

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Choi et al., "Particle Size Effects on Temperature-Dependent Performance of LiCoO2 in Lithium Batteries," J. Power Sources, vol. 158, (2006), pp. 1419-1424.
  • International Preliminary Report on Patentability, issued in PCT/US2010/000545, dated Aug. 23, 2011.
  • International Search Report, issued in PCT/US2010/000545, dated Apr. 9, 2010.
  • Jiang et al., "Effects of Particle Size and Electrolyte Salt on the Thermal Stability of Li0.5CoO2," Electroch. Acta, vol. 49, (2004), pp. 2661-2666.
  • Paulsen et al., "Core-Shell Cathode Material with Size-Dependent Composition," Electrochemical and Solid-State Letters, vol. 10, No. 4, (2007), pp. A101-A105.