Patents
US 8,671,567 B2#11596242 Most CitedActiveUnited States (USPTO)Utility

Method for manufacturing a probe for an electrical test

9Forward Citations (#11596242 Global)
0.8/yrCitation Velocity (#9916840 Global)
2.12Citation PageRank (#13195315 Global)
12Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for manufacturing a probed for an electrical test includes producing by a deposition technique a deposit including a probe main body portion made of a nickel-boron alloy and a probe tip portion projecting downward from the probe main body portion and made of a different conductive material from the probe main body portion. The method further includes annealing the deposit. The average grain diameter of the nickel-boron alloy is between 97 Å and 170 Å. The contained amount of boron is from 0.02 wt % to 0.20 wt %.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a probe for an electrical test, comprising steps of: producing by a deposition technique a deposit including a probe main body portion made of a nickel-boron alloy and a probe tip portion projecting downward from said probe main body portion and made of a different conductive material from that for said probe main body portion; and annealing said deposit produced, wherein the average grain diameter of said nickel-boron alloy is between 97 Å and 170 Å, and the contained amount of said boron is from 0.02 wt % to 0.20 wt %.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein said step of annealing includes a step of heating said deposit at a temperature of from 200° C. to 400° C.

  3. Claim 3Depends on #1

    The method according to claim 1 , wherein said step of annealing further includes a step of heating said

Technical Overview & Description