Hard-facing alloys having improved crack resistance
Abstract
Weld deposit compositions with improved crack resistance, improved wear resistance, and improved hardness are provided by controlling matrix grain size and balancing Titanium and/or Niobium with Carbon and/or Boron content. Additionally, the presence of coarse chromium carbides is drastically decreased to reduce the amount of check-cracking. Preferably, the weld deposit is produced from a flux-cored or metal-cored wire. The weld deposit characteristics include a matrix having a fine grain size, small evenly dispersed carbides within the matrix, and a small amount of Carbon in the matrix.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 4.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A weld deposit composition produced from a flux-cored welding wire consisting of, by percent mass: between 0.7% and 2.0% Carbon; between 0.1% and 0.5% Manganese; between 0.7% and 1.4% Silicon; between 6.0% and 11.0% Chromium; between 0.5% and 2.0% Molybdenum; between 2.0% and 8.0% sum of Niobium and Titanium; between 0.2% and 1.0% Vanadium; between 0.2% and 0.9% Boron; between 0.4% and 0.8% Copper; and a balance comprising Iron; wherein amounts of Titanium and Niobium are balanced with amounts of Carbon and Boron to form intermetallic carbides and borides that act as grain refiners; the ratio
- Claim 2Independent Claim
The weld deposit composition according to claim
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗