A process for preparing a polyazole with an inherent viscosity, measured in at least 96% sulfuric acid at 25° C., greater than 2.9 dl/g, comprising the steps of i) mixing one or more aromatic tetraamino compounds with one or more aromatic carboxylic acids or esters thereof which comprise at least two acid groups per carboxylic acid monomer, or mixing one or more aromatic and/or heteroaromatic diaminocarboxylic acids, in polyphosphoric acid to form a solution and/or dispersion ii) heating the mixture from step i) under inert gas to temperatures in the range from 120° C. to 350° C. to form the polyazole, wherein in step ii), a mixture having a concentration of polyphosphoric acid, calculated as P 2 O 5 (by acidimetric means), based on the total amount of H 3 PO 4 , polyphosphoric acid and water in the mixture, greater than 78.22%, is heated, the amounts of the components are selected in step i) such that the proportion by weight of the tetraamino compounds and of the aromatic carboxylic acids or esters thereof which comprise at least two acid groups per carboxylic acid monomer, or of the diaminocarboxylic acids of the mixture in step ii), based on the total weight of the mixture, is

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a polyazole with an inherent viscosity, measured in at least 96% sulfuric acid at 25° C., greater than 2.9 dl/g, comprising the steps of i) mixing one or more aromatic tetramino compounds with one or more aromatic carboxylic acids or esters thereof which comprise at least two acid groups per carboxylic acid monomer, or mixing one or more aromatic and/or heteroaromatic diaminocarboxylic acids, in polyphosphoric acid to form a solution and/or dispersion ii) heating the mixture from step i) under inert gas to temperatures in the range from 120° C. to 350° C. to form the po

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (17)

PatentTitleYearCitations
DE 1,024,646 BBohrlochgeraet—2
US 4,141,800 AElectrochemical gas detector and method of using same197953
WO 9,613,872 A1Proton conducting polymers—105
WO 9,904,445 A1Process for producing polybenzimidazole pastes and gels for use in fuel cells—31
WO 02,088,219 A1Proton-conducting membrane and use thereof—50
WO 03,022,412 A2Proton-conducting membrane and the use of the same—26
DE 10,213,540 A1Lösung aus Vinylphosphonsäure, Verfahren zur Herstellung einer Polymerelektrolytmembran aus Polyvinylphosphaonsäure und deren Anwendung in Brennstoffzellen—9
DE 10,246,459 A1Polymer electrolyte membrane for use, e.g. in fuel cells, obtained by heating a mixture of phosphonated aromatic polyazole monomers in polyphosphoric acid and then processing to form a self-supporting membrane—23
WO 2005/011039 A2Proton-conducting membrane and use thereof—9
US 2005147859 A1Mixture comprising phosphonic acid containing vinyl, polymer electrolyte membranes comprising polyvinylphoshphonic acid and the use thereof in fuel cells—57
US 2006008690 A1Proton conducting polymer membrane comprising phoshphonic acid groups containing polyazoles and the use thereof in fuel cells—60
US 7,288,603 B2Polybenzazole compound having sulfonic acid group and/or phosphonic acid group, resin composition containing the same, resin molding, solid polymer electrolyte membrane, solid polymer electrolyte membrane/electrode assembly and method of preparing assembly200719
US 2008050514 A1Proton-Conducting Membrane and the Use Thereof—14
WO 2008/031554 A1Process for producing a proton-conducting, polyazole-containing membrane—12
US 2010181697 A1Process for producing a proton-conducting, polyazole-containing membrane—10
US 2010216051 A1Proton-conducting polymer membrane comprising polyazole blends and its use in fuel cells—5
US 2011288187 A1Proton-conducting membrane and the use of the same—3

Non-Patent Literature (2)

  • International Preliminary Report on Patentability for PCT/EP2010/003671 mailed Aug. 2, 2011.
  • International Search Report for PCT/EP2010/003671 mailed Jan. 5, 2010.