Abstract

A method of servicing a wellbore comprising preparing a composition comprising a calcium aluminate cement, water, and a fluid loss additive wherein the fluid loss additive comprises an acid gelling polymer, placing the composition in the wellbore, and allowing the composition to set. A method of servicing a wellbore comprising placing into a wellbore having a bottom hole static temperature of greater than about 50° F. and/or a pH of from about 3 to about 9 a cement slurry comprising a calcium aluminate cement having an aluminum oxide content of greater than about 60 wt. % based on the total weight of the calcium aluminate cement and an acid-gelling polymer wherein the cement slurry has a fluid loss at 10 cc/10 min. to about 600 cc/30 min.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of servicing a wellbore comprising: preparing a composition comprising a calcium aluminate cement, water, and a fluid loss additive, wherein the calcium aluminate cement comprises aluminum oxide in an amount of greater than about 60 wt. % based on a total weight of the calcium aluminate cement and wherein the fluid loss additive comprises an acid gelling polymer; placing the composition in the wellbore; and allowing the composition to set, wherein the composition has a fluid loss of from about 10 cc/10 min. to about 600 cc/30 min. at a temperature of from about 50° F. to about 500° F.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the calcium aluminate cement has an aluminum oxide:calcium oxide ratio of from about 1:1 to about 4:1.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the composition has a pH in a range of fro

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,236,305 AMethod of acidizing wells196610
US 3,734,188 AWell cementing and stimulation method197313
US 4,015,991 ALow fluid loss cementing compositions containing hydrolyzed acrylamide/2-acrylamido-2-methylpropane sulfonic acid derivative copolymers and their use1977158
US 4,244,826 AGelled acidic well treating composition and process198135
US 4,466,893 AMethod of preparing and using and composition for acidizing subterranean formations198470
US 4,674,574 AFluid loss agents for oil well cementing composition1987120
US 4,683,952 AFluid loss control in oil field cements198711
US 5,340,397 ASet retarded ultra fine cement compositions and methods199479
US 5,346,012 AFine particle size cement compositions and methods1994304
US 5,588,488 ACementing multi-lateral wells1996254
US 5,913,364 AMethods of sealing subterranean zones1999220
US 5,975,206 AAcid gels for fracturing subterranean formations199973
US 6,110,271 AMethods for improved rheological control in cementitious systems2000118
US 6,167,967 B1Methods of sealing subterranean zones2001218
US 6,258,757 B1Water based compositions for sealing subterranean zones and methods2001220
US 6,497,283 B1Well cement additives, compositions and methods200239
US 2003008779 A1Compositions for treating subterranean zones penetrated by well bores—57
US 2003083204 A1Methods of treating subterranean zones penetrated by well bores—32
US 6,607,035 B1Preventing flow through subterranean zones200358
US 6,616,753 B2Methods and compositions for sealing subterranean zones200316
US 6,743,288 B2Well cement additives, compositions and methods200425
US 6,767,867 B2Methods of treating subterranean zones penetrated by well bores200448
US 6,770,604 B2High temperature viscosifying and fluid loss controlling additives for well cements, well cement compositions and methods200421
US 6,796,378 B2Methods of cementing high temperature wells and cement compositions therefor200431
US 6,822,061 B2Well cement additives, compositions and methods200416
US 2004262000 A1Cement compositions with improved fluid loss characteristics and methods of cementing in surface and subterranean applications—40
US 6,846,357 B2Methods of cementing high temperature wells and cement compositions therefor200531
US 6,846,420 B2Process for removing oil from solid materials recovered from a well bore200530

Non-Patent Literature (4)

  • "Recommended practice for testing well cements," ANSI/API Recommended Practice 10B-2 (Formerly 10B), Jul. 2005, First Edition, pp. 90-95 and title page, American Petroleum Institute.
  • Foreign communication from a related counterpart application-International Preliminary Report on Patentability, PCT/GB2011/001690, Jun. 12, 2013, 9 pages.
  • Foreign communication from a related counterpart application-International Search Report and Written Opinion, PCT/GB2011/001690, Mar. 22, 2012, 13 pages.
  • Norman, Lewis R., et al., "Temperature-stable acid-gelling polymers: laboratory evaluation and field results," Journal of Petroleum Technology, Nov. 1984, pp. 2011-2018, Society of Petroleum Engineers of AIME.