Abstract

A surface treatment solution for autodeposition coating treatment of a metallic material, which is an aqueous solution comprising at least one tannin, at least one crosslinking agent having a crosslinking group capable of thermosetting reaction with a phenolic hydroxyl group and/or a phenolic nucleus, ferric ions, soluble type elemental fluorine, and an oxidizing agent, wherein the solids mass concentration ratio of the tannin to the crosslinking agent is in the range of from 1:1 to 1:10, the molar concentration of the soluble type elemental fluorine is at least 3-fold the molar concentration of the ferric ions, and the pH of the solution is from 2 to 6. The surface treatment solution allows shorter process length as compared with conventional coating processes, generates less environmentally harmful by-products such as sludge, has excellent throwing power at the interior of a pocket structure, does not use environmentally harmful components such as chromium compounds, has corrosion resistance, and allows overcoating of a baking finish on the obtained coating film.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A surface treatment solution for autodeposition coating treatment of a metallic material, comprising an aqueous solution comprising: at least one tannin; at least one crosslinking agent having a crosslinking group capable of thermosetting reaction with a phenolic hydroxyl group and/or a phenolic nucleus; ferric ions; soluble elemental fluorine comprising hydrofluoric acid; at least one fluoride selected from the group consisting of cerium fluoride, yttrium fluoride, aluminum fluoride and strontium fluoride; said at least one fluoride having low solubility in an aqueous solution of hydrofluoric

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (17)

PatentTitleYearCitations
US 4,017,334 AProcess for treating aluminum cans197749
JP S53116240 AMethod of forming top coat of metal—6
US 4,338,140 ACoating composition and method198273
JP S61168673 AAuto-deposition composition—5
JP H0892540 AUrethane-based aqueous adhesive composition—9
US 5,868,820 AAqueous coating compositions and coated metal surfaces199953
JP 2000262967 ALow toxic precoated metallic plate excellent in corrosion resistance and coating film adhesibility—11
JP 2002501100 A水性プライマ−又は塗料—6
JP 2002266081 AChemical conversion treatment solution for pretreatment to coating and chemical conversion treated steel sheet for coating—11
US 6,525,112 B1Autodepositable prepolymer of epoxy- and OH-containing resin and hybrid isocyanate crosslinker200319
JP 2003176449 ACurable autodeposition coating film, autodeposition composition, coated metal substrate, and method for forming coating film on metal substrate—12
JP 2003301274 ASurface-treated metallic material—17
JP 2005015676 AComposition affording antifouling property, coating composition using the same and coated film using the coating composition—33
WO 2006/126560 A1Chemical treating liquid for metal and treating method—9
JP 2008013756 AComposition for imparting antifouling property and coating composition—13
US 2008230395 A1Metal surface treatment liquid for cation electrodeposition coating—36
WO 2009/147960 A1Surface treatment fluid for the autodeposition coating of metal materials and autodeposition coating process—3

Non-Patent Literature (1)

  • International Search Report for PCT/JP2009/059457, dated Jun. 23, 2009, 2 pages.