Methods for making environmental barrier coatings and ceramic components having CMAS mitigation capability
Abstract
Methods of making components having calcium magnesium aluminosilicate (CMAS) mitigation capability involving providing a component; applying an environmental barrier coating to the component, the environmental barrier coating having a separate CMAS mitigation layer including a CMAS mitigation composition selected from rare earth elements, rare earth oxides, zirconia, hafnia partially or fully stabilized with alkaline earth or rare earth elements, zirconia partially or fully stabilized with alkaline earth or rare earth elements, magnesium oxide, cordierite, aluminum phosphate, magnesium silicate, and combinations thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 19.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of making a component having CMAS mitigation capability comprising: providing a component, wherein the component comprises a ceramic matrix composite or a monolithic ceramic; applying an environmental barrier coating to the component, the environmental barrier coating comprising: a bond coat layer comprising silicon overlying the component; an optional silica layer overlying the bond coat layer; at least one transition layer overlying the bond coat layer or the optional silica layer comprising a composition selected from the group consisting of mullite, BSAS, and combinations thereof;
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 19 total)
References Cited — Backward Prior Art (35)
Non-Patent Literature (1)
- Office Action from corresponding JP Application No. 2009-236756, dated Jun. 4, 2013.