Abstract
Fabricating a semiconductor device includes: forming a gate trench in an epitaxial layer overlaying a semiconductor substrate; disposing gate material in the gate trench; forming a body in the epitaxial layer; forming a source in the body; forming an active region contact trench that has a varying trench depth; and disposing a contact electrode within the active region contact trench. Forming the active region contact trench includes performing a first etch to form a first contact trench depth associated with a first region, and performing a second etch to form a second contact trench depth associated with a second region. The first contact trench depth is substantially different from the second contact trench depth.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 29 · Forward citations: 4.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of fabricating a semiconductor device, comprising: forming a gate trench in an epitaxial layer overlaying a semiconductor substrate; disposing gate material in the gate trench; forming a body in the epitaxial layer; forming a source in the body; forming an active region contact trench that has a varying trench depth, including: performing a first etch to form a first contact trench depth associated with a first region; and performing a second etch to form a second contact trench depth associated with a second region; wherein the first contact trench depth is substantially different fr
- Claim 2Depends on #1
The method of claim 1 , wherein: performing the first etch includes: applying a first mask; and etching