Patents
US 8,633,040 B2#34058039 Most CitedActiveUnited States (USPTO)Utility

Method for synthesising semiconductor quantum dots

3Forward Citations (#34058039 Global)
0.2/yrCitation Velocity (#29194434 Global)
0.96Citation PageRank (#44680438 Global)
4Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention can be used for producing different luminescent materials and as a basis for producing subminiature light-emitting diodes, white light sources, single-electron transistors, nonlinear optical devices and photosensitive and photovoltaic devices. The inventive method for producing semiconductor quantum dots involves synthesizing nanocrystal nuclei from a chalcogen-containing precursor and a precursor containing a group II or IV metal using an organic solvent and a surface modifier. The method is characterized in that (aminoalkyl)trialkoxysilanes are used as the surface modifier, core synthesis is carried out at a permanent temperature ranging from 150 to 250 C for 15 seconds to 1 hour and in that the reaction mixture containing the nanocrystal is additionally treated by UV-light for 1-10 minutes and by ultrasound for 5-15 minutes.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for semiconductor quantum dot production on the basis of group II or group IV metal chalcogenides comprising: a nanocrystal core synthesis from a precursor containing a chalcogen and a precursor containing a group II or IV metal with the use of an organic solvent and a surface modifier wherein (aminoalkyl) trialkoxysilanes application are used as the modifiers and said cores are synthesized at a constant temperature ranging within 150° C.-250° C. for 15 seconds to 1 hour, and a reaction mixture containing the nanocrystal cores is additionally treated by UV-light for a duration of 1-10

  2. Claim 2Depends on #1

    The method of claim 1 wherein prior to UV-light and ultrasonic treatment of the reaction mixture, the semiconductor shell containing a group II metal chalcogenide is grown at a constant temper

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗