Patents
US 8,629,077 B2#47373021 Most CitedActiveUnited States (USPTO)Utility

Rare earth alumina particulate manufacturing method and application

1Forward Citations (#47373021 Global)
0.1/yrCitation Velocity (#48663605 Global)
0.97Citation PageRank (#43389019 Global)
20Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A rare earth alumina particulate composition manufacturing method and application are disclosed. The rare earth alumina of the invention is a particulate of porous structure with a molecular formula (RE x ,Al 1-x ) 2 O 3 , phase γ or γ+δ characterized by a particle size distribution ranging from 1 to 80 μm with a D 50 of 5 to 15 μm, a pore size distribution ranging from 0.4-200 nm with an average pore diameter of 8 to 30 nm, a pore volume (PV) raging from 0.5 to 1.2 cc/g and a fresh specific surface area (SA) ranging from 130 to 250 m 2 /g after calcination at 500-900° C. for 5 to 10 hours. The rare earth alumina retains a SA of greater than 60 m 2 /g after calcination at 1200° C. for 4 hours and greater than 40 m 2 /g after calcination at 1200° C. for 50 hours. There is no presence of the α phase or other impurity phases in the long-term aged samples. The rare earth alumina of the invention has a high thermal stability and is a fine three-way catalyst support material. The rare earth alumina is made using wet continuous coprecipitation with a static mixer and a tank reactor featuring simple operation, low cost and high feasibility in industrial production.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A calcined alumina catalyst support with at least one rare earth oxide as a stabilizer having a chemical formula (RE x ,Al 1-x ) 2 O 3 , in which, RE denotes one or more rare earth elements selected from the group: La, Ce, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er and Tm; the alumina catalyst support being characterized by a rare earth molar content x of 0.005 to 0.04, and after calcination at 1200° C. for 50 hours the alumina catalyst support comprises a surface area (SA) in excess of 30 m 2 /g and a theta phase absent the presence of any alpha phase.

  2. Claim 2Depends on #1

    The alumina catalyst support according to claim 1 wherein the rare earth alumina is characterized by a rare earth molar content x of 0.01 to 0.03.

  3. Claim 3Depends on #1

    The alumina catalyst support according to claim 1 wherein the rare earth alumina prior to calcination is character

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 2,620,314 ASpheroidal alumina1952182
US 3,903,020 AStabilized automotive exhaust gas catalyst197534
US 3,993,572 ARare earth containing catalyst composition1976129
US 4,170,573 ARare earth and platinum group metal catalyst compositions197955
US 4,868,150 ACatalyst support material containing lanthanides198949
US 5,155,085 AHeat resistant transition alumina and process for producing the same199233
US 5,397,758 AAlumina-based compositions and catalysts having high specific surface area199530
US 5,593,654 APreparation of stabilized alumina having enhanced resistance to loss of surface area at high temperatures199734
US 6,180,075 B1Exhaust gas catalyst200154
US 6,426,443 B1Catalytic process for the decomposition of perfluoroalkanes200215
US 2002160912 A1Composite oxide powder, catalyst and process for producing the same—41
US 2002187894 A1Catalyst material and a process for its preparation—9
US 2004127586 A1Stabilized transition alumina catalyst support from boehmite and catalysts made therefrom—31
US 2004138060 A1Stabilized alumina supports, catalysts made therefrom, and their use in partial oxidation—44
US 6,764,672 B2Thermally stable alumina particulates200424
US 2005265920 A1Supports and catalysts comprising rare earth aluminates, and their use in partial oxidation—49
WO 2006/070203 A1Thermally stable doped and undoped porous aluminum oxides and nanocomposite ce02-zro2 and al203 containing mixed oxides—9
US 7,162,963 B2Adjustable singulating brush assembly and method of singulating seeds200716
US 2007161714 A1Fischer-tropsch catalysts—12
US 2008096760 A1Composite Oxides Or Hydroxides Comprising Alumina And Zirconia For Automotive Catalyst Applications And Method Of Manufacturing—11

Non-Patent Literature (4)

  • Nair et al., "Pore Structure Evolution of Lanthana-Alumina Systems Prepared through Coprecipitation", J. Am. Ceram. Soc. 83 (8) 1942-46 (2000).
  • Wachowski et al., "Studies of physicochemical and surface properties of alumina modified with rare-earth oxides I. Preparation, structure and thermal stability", Materials Chemistry and Physics, 37 (1994) 29-38.
  • Wachowski et al., "Studies of physicochemical and surface properties of alumina modified with rare-earth oxides. II. Porous Structure", Catalysis Letters 32 (1995) 123-130.
  • Yamamoto et al., "Structures and Acid-Base Properties of La/Al2O3-Role of La Addition to Enhance Thermal stability of gamma-Al2O3", Chem. Mater. 2003, 15, 4830-4840.