Patents
US 8,629,065 B2#27313289 Most CitedActiveUnited States (USPTO)Utility

Growth of planar non-polar {10-10} M-plane gallium nitride with hydride vapor phase epitaxy (HVPE)

4Forward Citations (#27313289 Global)
0.3/yrCitation Velocity (#23587324 Global)
1.04Citation PageRank (#39414520 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of growing planar non-polar m-plane III-Nitride material, such as an m-plane gallium nitride (GaN) epitaxial layer, wherein the III-Nitride material is grown on a suitable substrate, such as an m-plane Sapphire substrate, using hydride vapor phase epitaxy (HVPE). The method includes in-situ pretreatment of the substrate at elevated temperatures in the ambient of ammonia and argon, growing an intermediate layer such as an aluminum nitride (AlN) or aluminum-gallium nitride (AlGaN) on the annealed substrate, and growing the non-polar m-plane III-Nitride epitaxial layer on the intermediate layer using HVPE. Various alternative methods are disclosed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of growing a planar non-polar Gallium-Nitride epitaxial film, comprising: providing an m-plane sapphire substrate; cleaning and annealing the m-plane sapphire substrate in a hydrogen environment at a temperature of approximately 900° C. for a duration of approximately 10 to 20 minutes; nitridizing the annealed m-plane sapphire substrate in an ammonia environment at a temperature of approximately 600° C. for approximately 3 to 10 minutes; growing an intermediate layer of Aluminum Nitride (AlN) or Aluminum Gallium Nitride (AlGaN) at a temperature of approximately 600° C. on the nitridiz

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 5,923,950 AMethod of manufacturing a semiconductor light-emitting device199955
US 6,045,626 ASubstrate structures for electronic devices2000278
US 6,064,078 AFormation of group III-V nitride films on sapphire substrates with reduced dislocation densities2000134
US 6,069,021 AMethod of growing group III nitride semiconductor crystal layer and semiconductor device incorporating group III nitride semiconductor crystal layer2000185
US 6,072,197 ASemiconductor light emitting device with an active layer made of semiconductor having uniaxial anisotropy2000347
US 6,156,581 AGaN-based devices using (Ga, AL, In)N base layers2000433
US 6,201,262 B1Group III nitride photonic devices on silicon carbide substrates with conductive buffer interlay structure2001514
US 6,218,269 B1Process for producing III-V nitride pn junctions and p-i-n junctions200149
JP 2001342100 AManufacturing method of substrate for epitaxial growth and manufacturing method of semiconductor device using substrate for this epitaxial growth—54
US 2002074552 A1Gallium nitride materials and methods—101
US 2002085603 A1Gallium nitride semiconductor light emitting device having multi-quantum-well structure active layer, and semiconductor laser light source device—223
US 6,440,823 B1Low defect density (Ga, Al, In)N and HVPE process for making same2002203
US 6,468,882 B2Method of producing a single crystal gallium nitride substrate and single crystal gallium nitride substrate2002166
US 2002187356 A1Gallium nitride materials and methods—61
US 6,573,164 B2Method of epitaxially growing device structures with sharp layer interfaces utilizing HVPE200311
US 6,613,143 B1Method for fabricating bulk GaN single crystals200368
US 6,616,757 B1Method for achieving low defect density GaN single crystal boules200359
US 6,627,552 B1Method for preparing epitaxial-substrate and method for manufacturing semiconductor device employing the same200390
US 2003198837 A1Non-polar a-plane gallium nitride thin films grown by metalorganic chemical vapor deposition—104
WO 03,089,694 A1NON-POLAR (A1,B,In,Ga) QUANTUM WELL AND HETEROSTRUCTURE MATERIALS AND DEVICES—36
US 6,656,285 B1Reactor for extended duration growth of gallium containing single crystals200333
US 6,656,272 B2Method of epitaxially growing submicron group III nitride layers utilizing HVPE200320
US 6,660,083 B2Method of epitaxially growing device structures with submicron group III nitride layers utilizing HVPE200327
EP 1,385,196 A2Method of producing a Group III nitride semiconductor crystal—26
US 6,706,119 B2Apparatus for epitaxially growing semiconductor device structures with submicron group III nitride layer utilizing HVPE200427
US 2004094773 A1Nitride semiconductor growth method, nitride semiconductor substrate and nitride semiconductor device—40

Non-Patent Literature (5)

  • "Brief Communication re Oral Proceedings dated Dec. 11, 2012, European Patent Application No. 09790542.6".
  • "Communication pursuant to Article 94(3) EPC dated Dec. 15, 2011, European Patent Application No. 09790542.6".
  • "Communication pursuant to Article 94(3) EPC dated Jul. 22, 2011, European Patent Application No. 09790542.6".
  • "Communication pursuant to Rules 161(1) and 162 EPC dated Mar. 1, 2011, European Patent Application No. 09790542.6".
  • "Communication under Rule 71(3) EPC dated Dec. 19, 2012, European Patent Application No. 09790542.6".