Patents
US 8,618,440 B2#45124685 Most CitedActiveUnited States (USPTO)Utility

Sprayed weld strip for improved weldability

2Forward Citations (#45124685 Global)
0.1/yrCitation Velocity (#39041485 Global)
0.88Citation PageRank (#49311711 Global)
47Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for welding to a superalloy material without causing cracking of the material. The method includes the steps of depositing a weld strip ( 18 ) of a weldable material onto a superalloy substrate material ( 12 ) using a spray deposition process ( 20 ) and then forming a weldment ( 26 ) to the weld strip. None or a controlled amount of the substrate material ( 12 ) is melted during the weld in order to maintain the concentration of strengthening elements in the local melt within a zone of weldability. The spray deposition process may be a thermal process such as HVOF or a cold spray process. A groove ( 16 ) may be formed in a surface ( 10 ) of the superalloy substrate material to receive the weld strip. A diffusion heat treatment step may be used to improve adhesion between the weld strip and the superalloy material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 47 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for joining to a nickel-based superalloy substrate material having a composition outside of a zone of weldability defined as a concentration of strengthening elements wherein a sum of a concentration of aluminum plus one-half a concentration of titanium in the material is less than 3 w/o, the method comprising: applying to the superalloy substrate material a weld strip of a material having a composition within the zone of weldability using a spray deposition process; and forming a fusion weld to the weld strip.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein none of the superalloy substrate material melts during the step of forming a fusion weld.

  3. Claim 3Depends on #1

    The method of claim 1 , further comprising melting a portion of the superalloy substrate material during the step of forming a fusion weld while maintaining

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (47)

PatentTitleYearCitations
US 4,213,026 AAge hardenable nickel superalloy welding wires containing manganese198029
US 4,231,795 AHigh weldability nickel-base superalloy198015
US 4,336,312 AWeldable nickel base cast alloy for high temperature applications and method198238
US 4,804,815 AProcess for welding nickel-based superalloys1989106
US 4,938,805 ANovel cobalt-base superalloy and cast and welded industrial gas turbine components thereof and method199017
US 4,965,095 AMethod for refurbishing used jet engine hot section airfoils199053
US 4,973,366 AInsert material for solid phase diffusion welding for nickel base superalloy and method therefor199019
US 5,040,718 AMethod of repairing damages in superalloys199141
US 5,106,010 AWelding high-strength nickel base superalloys199280
US 5,142,778 AGas turbine engine component repair199282
US 5,302,414 AGas-dynamic spraying method for applying a coating1994628
US 5,374,319 AWelding high-strength nickel base superalloys199477
US 5,509,980 ACyclic overageing heat treatment for ductility and weldability improvement of nickel-based superalloys199642
US 5,554,837 AInteractive laser welding at elevated temperatures of superalloy articles1996128
US 5,302,414 B1Gas-dynamic spraying method for applying a coating1997620
US 5,732,467 AMethod of repairing directionally solidified and single crystal alloy parts1998113
US 5,785,775 AWelding of gamma titanium aluminide alloys199835
US 5,897,801 AWelding of nickel-base superalloys having a nil-ductility range1999132
US 6,049,978 AMethods for repairing and reclassifying gas turbine engine airfoil parts2000126
US 6,054,672 ALaser welding superalloy articles200052
US 6,084,196 AElevated-temperature, plasma-transferred arc welding of nickel-base superalloy articles200058
US 6,191,379 B1Heat treatment for weld beads2001117
US 6,302,649 B1Superalloy weld composition and repaired turbine engine component200137
US 6,333,484 B1Welding superalloy articles200192
US 6,354,799 B1Superalloy weld composition and repaired turbine engine component200220
US 6,364,971 B1Apparatus and method of repairing turbine blades200256
US 6,376,801 B1Gas turbine component refurbishment apparatus and repair method200255
US 6,468,367 B1Superalloy weld composition and repaired turbine engine component200233

Non-Patent Literature (5)

  • "CM-247 LC: for turbine blades and vanes"; [online]; [retrieved on Oct. 19, 2006]; 3 pages; Retrieved from http://www.c-mgroup.com/spec-sheets/CM-247.htm.
  • "CM-247 LC: for turbine blades and vanes"; [online]; [retrieved on Oct. 19, 2006]; 3 pages; Retrieved from http://www.c-mgroup.com/spec—sheets/CM—247.htm.
  • "Nickel Base DS: A selection guide to common vacuum melted alloys"; [online]; [retrieved on Oct. 19, 2006; 2 pages; Retrieved from http://www.cm-group.com/vacuum-melt-index/nickel-base.ds.htm.
  • "Nickel Base DS: A selection guide to common vacuum melted alloys"; [online]; [retrieved on Oct. 19, 2006; 2 pages; Retrieved from http://www.cm-group.com/vacuum—melt—index/nickel—base.ds.htm.
  • "Superalloy"; [online]; [retrieved on Aug. 28, 2006]; 3 pages; Retrieved from http://en.wikipedia.org/wiki/Superalloy.