Patents
US 8,618,239 B2#62105687 Most CitedActiveUnited States (USPTO)Utility

Solid-stage polymerization system for a liquid crystalline polymer

1Forward Citations (#62105687 Global)
0.1/yrCitation Velocity (#49696112 Global)
0.74Citation PageRank (#62105687 Global)
49Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A multi-stage process for forming a liquid crystalline polymer is provided. More particularly, the process includes acetylating one or more precursor monomers and melt-polymerizing the acetylated monomers to form a prepolymer in the form of a solid particulate material. Thereafter, the prepolymer is solid-state polymerized in a fluidized bed reactor that contains a porous surface (e.g., bed, plate, grate, etc.) on which the prepolymer is supported. While supported by this porous surface, the prepolymer can become “fluidized” with a heated stream of a gas (e.g., nitrogen). In this manner, a sufficient degree of turbulence is created to distribute heat evenly around the prepolymer and cause it to rapidly reach the target reaction temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 49 · Forward citations: 1.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for forming a thermotropic, wholly aromatic liquid crystalline polymer, the method comprising: acetylating one or more precursor monomers for the liquid crystalline polymer; melt-polymerizing the acetylated monomers to form a liquid crystalline prepolymer that is in the form of a solid particulate material; feeding the prepolymer into a fluidized bed reactor; and supplying a heated gaseous stream into the fluidized bed to polymerize the prepolymer for a certain reaction time period, the heated gaseous stream increasing the temperature of the prepolymer at a rate of about 2.0° C. per m

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the heated gaseous stream increases the temperature of the prepolymer at

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (49)

PatentTitleYearCitations
US 3,728,309 AProgressive heating in polyester condensations197320
US 3,840,632 ASolid phase polymerization of strain hardened polyesters197415
US 4,075,173 AProcess for the production of aromatic polyesters from hydroxybenzoic acid and products thereof197896
US 4,083,829 AMelt processable thermotropic wholly aromatic polyester1978254
US 4,161,470 APolyester of 6-hydroxy-2-naphthoic acid and para-hydroxy benzoic acid capable of readily undergoing melt processing1979400
US 4,184,996 AMelt processable thermotropic wholly aromatic polyester1980129
US 4,219,461 APolyester of 6-hydroxy-2-naphthoic acid, para-hydroxy benzoic acid, aromatic diol, and aromatic diacid capable of readily undergoing melt processing1980147
US 4,256,624 APolyester of 6-hydroxy-2-naphthoic acid, aromatic diol, and aromatic diacid capable of undergoing melt processing1981129
US 4,279,803 APolyester of phenyl-4-hydroxybenzoic acid and 4-hydroxybenzoic acid and/or 6-hydroxy-2-naphthoic acid capable of forming an anisotropic melt198163
US 4,318,841 APolyester of 6-hydroxy-2-naphthoic acid, para-hydroxy benzoic acid, terephthalic acid, and resorcinol capable of readily undergoing melt processing to form shaped articles having increased impact strength198284
US 4,330,457 APoly(ester-amide) capable of forming an anisotropic melt phase derived from 6-hydroxy-2-naphthoic acid, dicarboxylic acid, and aromatic monomer capable of forming an amide linkage198299
US 4,337,190 APolyester of 6-hydroxy-2-naphthoic acid and meta-hydroxy benzoic acid capable of readily undergoing melt processing198267
US 4,339,375 APoly(ester-amide) capable of forming an anisotropic melt phase derived from p-hydroxybenzoic acid, 2,6-dihydroxynaphthalene, carbocyclic dicarboxylic acid, aromatic monomer capable of forming an amide linkage, and, optionally, additional aromatic diol198264
US 4,351,917 APoly(ester-amide) capable of forming an anisotropic melt phase derived from 6-hydroxy-2-naphthoic acid, aromatic monomer capable of forming an amide linkage, and other aromatic hydroxyacid198295
US 4,351,918 APoly(ester-amide) capable of forming an anisotropic melt phase derived from 6-hydroxy-2-naphthoic acid, other aromatic hydroxyacid, carbocyclic dicarboxylic acid, and aromatic monomer capable of forming an amide linkage198296
US 4,355,132 AAnisotropic melt phase forming poly(ester-amide) derived from p-hydroxybenzoic acid, 2,6-naphthalenedicarboxylic acid, aromatic monomer capable of forming an amide linkage, and, optionally, hydroquinone and additional carbocyclic dicarboxylic acid1982101
US 4,355,134 AWholly aromatic polyester capable of forming an anisotropic melt phase at an advantageously reduced temperature198258
US 4,375,530 APolyester of 2,6-naphthalene dicarboxylic acid, 2,6-dihydroxy naphthalene, terephthalic acid, and hydroquinone capable of forming an anisotropic melt198387
US 4,393,191 APreparation of aromatic polyesters by direct self-condensation of aromatic hydroxy acids198374
US 4,421,908 APreparation of polyesters by direct condensation of hydroxynaphthoic acids, aromatic diacids and aromatic diols198359
US 4,429,105 AProcess for preparing a polyester of hydroxy naphthoic acid and hydroxy benzoic acid198462
US 4,434,262 AMelt processable blend of a low molecular weight liquid crystalline compound and a polyolefin or polyester198458
US 4,473,682 AMelt processable polyester capable of forming an anisotropic melt comprising a relatively low concentration of 6-oxy-2-naphthoyl moiety, 4-oxybenzoyl moiety, 4,4'-dioxybiphenyl moiety, and terephthaloyl moiety1984115
US 4,522,974 AMelt processable polyester capable of forming an anisotropic melt comprising a relatively low concentration of 6-oxy-2-naphthoyl moiety-4-benzoyl moiety, 1,4-dioxyphenylene moiety, isophthaloyl moiety and terephthaloyl moiety1985110
US 4,778,858 APreparation of thermoplastic resin composition by solid state polymerization198849
US 4,994,546 AProcess for preparing bisphenol polyarylates19914
US 5,204,443 AMelt processable poly(ester-amide) capable of forming an anisotropic melt containing an aromatic moiety capable of forming an amide linkage199369
US 5,214,073 APorous, crystallized, aromatic polycarbonate prepolymer, a porous, crystallized aromatic polycarbonate, and production methods199331
US 5,541,240 AMethod for making blends of liquid crystalline and isotropic polymers199657

Non-Patent Literature (1)

  • Search Report and Written Opinion for PCT/US2012/057213 dated Apr. 16, 2013, 10 pages.