Alumina ceramic for spark plug insulator
Abstract
A spark plug includes an insulator formed of a ceramic material. The ceramic material comprises Al 2 O 3 in an amount of 98.00 wt % to 99.50 wt %; Group 2 oxides in an amount of 0.16 wt % to 0.70 wt %; SiO 2 in an amount of 0.25 wt % to 0.75 wt %, Group 4 oxides in an amount of 0.01 wt % to 0.16 wt %, Group 1 oxides in an amount less than 0.0060 wt %, and P 2 O 5 in an amount of less than 0.0040 wt %. The Al 2 O 3 is formed of particles having a D50 median particle size by volume of 1.2 μm to 1.8 μm. The ceramic material is pressed, sintered, and formed to a predetermined shape. The sintered ceramic material includes a glass phase comprising the Al 2 O 3 , Group 2 oxides, and SiO 2 . The sintered ceramic material also includes secondary crystals of calcium hexa-aluminate (CaAl 12 O 19 ) spinel (MgAl 2 O 4 ), anorthite (CaAl 2 Si 2 O 8 ), and mullite (Al 6 Si 2 O 13 ).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 7.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A ceramic material for an insulator of a spark plug comprising, in weight percent (wt %) of said ceramic material, aluminum oxide (Al 2 O 3 ) in an amount of 98.00 wt % to 99.50 wt %; at least one oxide of a Group 2 alkaline earth metal (Group 2 oxide) in an amount of 0.16 wt % to 0.70 wt %; said at least one Group 2 oxide including at least one of calcium oxide (CaO), magnesium oxide (MgO), beryllium oxide (BeO), strontium oxide (SrO), barium oxide (BaO), and radium oxide (RaO); silicon dioxide (SiO 2 ) in an amount of 0.25 wt % to 0.75 wt %; at least one oxide of a Group 4 transitional metal
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗