Method for manufacturing semiconductor device
Abstract
Disclosed is a method for manufacturing a semiconductor device, which provides an isolation region in which a dense silicon oxide film is formed in a trench that requires high aspect ratio. The method includes forming an isolation trench using, as an etching mask, a nitride mask film formed on a substrate, forming a liner nitride film in the isolation trench, depositing a flowable silazane compound by a CVD method such that the height of the flowable silazane compound is higher than the upper surface of the nitride mask film from the upper portion of the trench, performing heat treatment under an oxidizing atmosphere to convert the flowable silazane compound film into a silicon oxide film and simultaneously densifying therefore, and planarizing the silicon oxide film to the height of the upper surface of the nitride mask film.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for manufacturing a semiconductor device, comprising: etching a semiconductor substrate using a silicon nitride mask film formed on the semiconductor substrate as a mask to form a first isolation trench corresponding to a first isolation region; forming a liner silicon nitride film on at least an inner surface of the first isolation trench; depositing a flowable silazane compound by a CVD method such that the first isolation trench is filled with the flowable silazane compound by overfilling up to a height higher than the upper surface of the silicon nitride mask film in the vicinity
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (8 of 8 total)
References Cited — Backward Prior Art (2)
Non-Patent Literature (1)
- Chung, et al., "Novel Shallow Trench Isolation Process Using Flowable Oxide CVD for Sub-100nm DRAM", IEDM, 2002, pp. 233-236.