Patents
US 8,575,474 B2#42855662 Most CitedActiveUnited States (USPTO)Utility

Solar cell contacts containing aluminum and at least one of boron, titanium, nickel, tin, silver, gallium, zinc, indium and copper

2Forward Citations (#42855662 Global)
0.1/yrCitation Velocity (#38964690 Global)
0.95Citation PageRank (#45194669 Global)
44Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Formulations and methods of making solar cell contacts and cells therewith are disclosed. In general, the invention provides a solar cell comprising a contact made from a mixture wherein, prior to firing, the mixture comprises at least one aluminum source, at least one source of a metal including one or more of boron, titanium, nickel, tin, gallium zinc, indium, and copper, and about 0.1 to about 10 wt % of a glass component. Within the mixture, the overall content of aluminum is about 50 wt % to about 85 wt % of the mixture, and the overall combined content of boron, nickel, tin, silver, gallium, zinc, indium, copper, is about 0.05 to about 40 wt % of the mixture.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 44 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A solar cell comprising a contact made from a mixture wherein, prior to firing, the mixture comprises: a. an aluminum source, wherein the content of aluminum is about 50 to about 85 wt % of the mixture, b. sources of at least two additional metals selected from the group consisting of boron, titanium, nickel, tin, silver, gallium, zinc, indium, copper, mixtures thereof, and alloys thereof, wherein each of the two additional metals is present in an amount of about 0.3 to about 10 wt % of the mixture; and c. about 0.1 to about 10 wt % of a lead-free and cadmium-free glass component, wherein the

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

References Cited — Backward Prior Art (44)

PatentTitleYearCitations
US 3,900,945 AOrganic semiconductor solar cell197543
US 4,070,517 ALow fired conductive compositions197839
US 4,088,502 ACorrosion resistant castable refractory mix197834
US 4,163,678 ASolar cell with improved N-region contact and method of forming the same197942
US 4,235,644 AThick film silver metallizations for silicon solar cells198063
US 4,492,813 AAmorphous silicon solar cell198522
US 4,703,553 ADrive through doping process for manufacturing low back surface recombination solar cells198786
US 4,899,704 ASelf-lubricating bearing19908
US 5,074,920 APhotovoltaic cells with improved thermal stability199141
EP 0,468,382 A1Electric conductor material for solar cell—8
US 5,178,685 AMethod for forming solar cell contacts and interconnecting solar cells1993245
US 5,584,941 ASolar cell and production process therefor199643
US 5,645,765 ALead-free conductive paste1997144
US 5,922,627 ALow resistivity palladium-silver compositions199915
US 5,928,438 AStructure and fabrication process for self-aligned locally deep-diffused emitter (SALDE) solar cell1999203
US 5,942,048 APhotovoltaic element electrode structure thereof and process for producing the same1999124
US 6,096,968 ASolar cell with a back-surface field2000102
US 6,262,359 B1Aluminum alloy back junction solar cell and a process for fabrication thereof2001125
US 2002005507 A1Conductive paste and printed wiring board using the same—33
US 6,402,839 B1System for stabilizing dendritic web crystal growth20028
US 6,469,243 B2Dye-sensitizing solar cell, method for manufacturing dye-sensitizing solar cell and solar cell module200263
JP 2003069056 APaste composition and solar battery using the same—62
US 6,576,391 B1Photosensitive paste a plasma display, and a method for the production thereof200328
US 6,626,993 B2Method for stabilizing dendritic web crystal growth20037
US 6,692,981 B2Method of manufacturing a solar cell200441
US 6,695,903 B1Dopant pastes for the production of p, p+, and n, n+ regions in semiconductors2004131
US 6,710,239 B2Solar cell, interconnector for solar cell, and solar cell string200442
US 6,737,340 B2Method and apparatus for self-doping contacts to a semiconductor200422

Non-Patent Literature (5)

  • ASM 5005 Aluminum Alloy specification, ASM 2002.
  • English Translation of JP 2003-069056, published Mar. 7, 2003, 15 pages.
  • English Translation of JP 2005-079143, published Mar. 24, 2005, 20 pages.
  • Extended European Search Report, Application No. 06846462 dated Jun. 15, 2012, Applicant-Ferro Corporation, nine pages.
  • Krause et al., "Determination of aluminum diffusion parameters in silicon", journal of applied physics, 2002.