Methods for manufacturing liquid ejecting head and piezoelectric element, liquid ejecting head, liquid ejecting apparatus, and piezoelectric element
Abstract
A method for manufacturing a piezoelectric element comprising forming a titanium film containing titanium; forming a platinum film containing platinum on the titanium film; forming a piezoelectric precursor film containing bismuth, lanthanum, iron and manganese on the platinum film; crystallizing the piezoelectric precursor film to form a piezoelectric layer by firing the piezoelectric precursor film in an atmosphere of an inert gas; and forming an electrode on the piezoelectric layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 43 · Forward citations: 0.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for manufacturing a piezoelectric element, comprising: forming a titanium film comprising titanium; forming a platinum film comprising platinum on the titanium film; forming a piezoelectric precursor film comprising bismuth, lanthanum, iron, and manganese on the platinum film; crystallizing the piezoelectric precursor film to form a piezoelectric layer by firing the piezoelectric precursor film in an atmosphere of an inert gas; and forming an electrode on the piezoelectric layer.
- Claim 2Depends on #1
The method according to claim 1 , wherein the inert gas is nitrogen.
- Claim 3Independent Claim
A method for manufacturing a liquid ejecting head comprising a pressure generating chamber communicating with a nozzle aperture and a piezoelectric element allowing the pressure generating chamber to change pressure, the method comprising: f
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (43)
Non-Patent Literature (5)
- EESR mailed on Jun. 20, 2011 in European Patent Application No. 11157439.8, for Seiko Epson Corporation.
- Machine Translation of JP2009113419A.
- Singh. S.K., Room temperature ferroelectric properties of Mn-substituted BiFe03 thin films deposited on Pt electrodes using chemical solution deposition, Appl. Phys. Lett. 88, 262908 (2006), Paragraphs 3-4.
- Wu, Jiagang, and John Wang. "Effects of SrRuO3 buffer layer thickness on mulitiferroic (Bi0.90La0.10)(Fe0.95Mn0.05)O3 thin films." Journal of Applied Physics 106.5 (2009): 054115.
- Zhang, Shan-Tao, Preparation, structures, and multiferroic properties of single phase Bi1 -xLaxFe03 (x=0-0.40) ceramics, J. Appl. Phys. 100, 114108 (2006), Paragraph 1.