A copper interconnect line formed on a passivation layer is protected by a copper-containing material layer including a group III element, a group IV element, a group V element or combinations thereof.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An integrated circuit device, comprising: a semiconductor substrate; a passivation layer overlying the semiconductor substrate; a polymer layer overlying the passivation layer; an interconnect line formed between the passivation layer and the polymer layer, the interconnect line extending over a top surface of the passivation layer; and a protection layer formed between the interconnect line and the polymer layer; wherein the protection layer is a copper-containing material layer comprising at least one of a group III element, a group IV element and a group V element.

  2. Claim 2Depends on #1

    The integrated circuit device of claim 1 , wherein the protection layer is a CuGeN layer.

  3. Claim 3Depends on #1

    The integrated circuit device of claim 1 , wherein the copper-containing material layer comprises at least one of germanium (Ge), silicon

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
JP H05335313 AManufacture of indium bump—48
US 5,466,635 AProcess for making an interconnect bump for flip-chip integrated circuit including integral standoff and hourglass shaped solder coating1995143
JP 2000228420 ASemiconductor device and manufacture thereof—61
US 6,218,281 B1Semiconductor device with flip chip bonding pads and manufacture thereof2001143
US 6,229,220 B1Bump structure, bump forming method and package connecting body2001221
US 2002185733 A1Barrier cap for under bump metal—46
US 6,500,750 B1Semiconductor device and method of formation200256
US 6,578,754 B1Pillar connections for semiconductor chips and method of manufacture2003206
US 6,592,019 B2Pillar connections for semiconductor chips and method of manufacture2003123
US 6,605,528 B1Post passivation metal scheme for high-performance integrated circuit devices200374
US 6,818,545 B2Low fabrication cost, fine pitch and high reliability solder bump2004158
US 6,853,076 B2Copper-containing C4 ball-limiting metallurgy stack for enhanced reliability of packaged structures and method of making same200585
US 6,917,119 B2Low fabrication cost, high performance, high reliability chip scale package200558
US 7,064,436 B2Semiconductor device and method of fabricating the same200657
US 2006292851 A1Circuitry component and method for forming the same—76
US 2007232051 A1Method for forming metal bumps—20
US 2008138624 A1Barrier layer, composite article comprising the same, electroactive device, and method—44
US 7,391,112 B2Capping copper bumps200855
TW 200,929,435 AIntegrated circuit structures and methods for forming the same—1
US 2010041234 A1Process For Restoring Dielectric Properties—26
US 2010090318 A1Backside Connection to TSVs Having Redistribution Lines—53

Non-Patent Literature (2)

  • Liu, C.S. et al., Self Aligned CuGeN Process for 32/22nm Nodes and Beyond, IEEE 987-1-4244-1911-1/08, pp. 199-201.
  • U.S. Appl. No. 12/786,698, filed May 25, 2010 entitled "Self-Aligned Protection Layer For Copper Post Structure", Chung-Shi Liu et al. (Not Yet Published).