Abstract

Semiconductor devices and methods for making such devices are described. The semiconductor devices contain dielectric layers that have been deposited and/or flowed by the application of microwave energy (“MW dielectric layers”). The dielectric layers can be made by providing a substrate in a reaction chamber, flowing a precursor gas mixture (containing atoms that react to form a dielectric material) in the reaction chamber, and then subjecting the gas mixture to microwave energy at a frequency and power density sufficient to cause the atoms of the precursor gas mixture to react and deposit to form a dielectric layer on the substrate. As well, the devices can be made by applying microwave energy to an already-deposited dielectric film at a frequency and power density sufficient to cause the atoms of the deposited dielectric material to flow. Using microwave energy permits the dielectric layer to be formed using low temperature processing, providing several benefits to the semiconductor device along with process flow efficiency and low cost. Other embodiments are described.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for making a dielectric layer, comprising: providing a substrate in a deposition chamber, wherein the upper surface of the substrate comprises a silicide-containing conductive material, a semiconductor material, or an insulating material; providing a precursor gas mixture in the deposition chamber, the precursor gas mixture containing atoms that react to form a dielectric material; and providing microwave energy at a frequency sufficient to cause the atoms of the precursor gas mixture to react and deposit a BPTEOS or BPSG dielectric layer on a portion of the substrate.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the time for the reaction ranges up to about 120 minutes.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the dielectric layer comprises a low-k gate dielectric material.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (14)

PatentTitleYearCitations
US 4,737,379 APlasma deposited coatings, and low temperature plasma method of making same1988489
US 4,785,763 AApparatus for the formation of a functional deposited film using microwave plasma chemical vapor deposition process198833
US 5,030,476 AProcess and apparatus for the formation of a functional deposited film on a cylindrical substrate by means of microwave plasma chemical vapor deposition199135
US 5,514,217 AMicrowave plasma CVD apparatus with a deposition chamber having a circumferential wall comprising a curved moving substrate web and a microwave applicator means having a specific dielectric member on the exterior thereof1996105
US 5,637,358 AMicrowave plasma chemical vapor deposition process using a microwave window and movable, dielectric sheet199727
US 5,643,365 AMethod and device for plasma vapor chemical deposition of homogeneous films on large flat surfaces199730
TW 415,009 BTwo-stage fabrication method of void free dielectrics20001
US 6,200,651 B1Method of chemical vapor deposition in a vacuum plasma processor responsive to a pulsed microwave source200157
US 2003152700 A1Process for synthesizing uniform nanocrystalline films—45
US 2004023140 A1Light-receiving member, image-forming apparatus, and image-forming method—16
US 2004238104 A1Apparatus and method for deposition of protective film for organic electroluminescence—25
US 2005156285 A1Low k and ultra low k SiCOH dielectric films and methods to form the same—45
US 7,589,028 B1Hydroxyl bond removal and film densification method for oxide films using microwave post treatment200924
US 2010079203 A1Semiconductor Device—11

Non-Patent Literature (1)

  • Taiwan Intellectual Property Office, Search Report dated Aug. 27, 2013 for Taiwan Application No. 100106787.