Conformal layers by radical-component CVD
Abstract
Methods, materials, and systems are described for forming conformal dielectric layers containing silicon and nitrogen (e.g., a silicon-nitrogen-hydrogen (Si—N—H) film) from a carbon-free silicon-and-nitrogen precursor and radical-nitrogen precursor. The carbon-free silicon-and-nitrogen precursor is predominantly excited by contact with the radical-nitrogen precursor. Because the silicon-and-nitrogen film is formed without carbon, the conversion of the film into hardened silicon oxide is done with less pore formation and less volume shrinkage. The deposited silicon-and-nitrogen-containing film may be wholly or partially converted to silicon oxide which allows the optical properties of the conformal dielectric layer to be selectable. The deposition of a thin silicon-and-nitrogen-containing film may be performed at low temperature to form a liner layer in a substrate trench. The low temperature liner layer has been found to improve the wetting properties and allows flowable films to more completely fill the trench.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 6.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of forming a conformal silicon-and-nitrogen-containing layer on a patterned substrate in a substrate processing region in a substrate processing chamber, the method comprising: mixing a carbon-free silicon-and-nitrogen-containing precursor with a radical-nitrogen precursor, wherein the carbon-free silicon-and-nitrogen-containing precursor is predominantly excited by contact with the radical-nitrogen precursor; and depositing a conformal silicon-and-nitrogen-containing layer having a conformal layer thickness on the patterned substrate, wherein the patterned substrate comprises a subst
- Claim 2Depends on #1
The method of claim 1 wherein a conformal deposition pressure in the substrate processing region during deposition of the conformal silicon-and-nitrogen-containing film is below or about 200 mTorr.
- Claim 3Independent Claim
Th
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗