Pressureless polymer pipe, a compositon therefore, and a process for preparing it
Abstract
A pressureless polymer pipe, a composition therefore, and a process of preparing the composition are described. The pipe is characterized in that the polymer comprises a propylene polymer composition where the propylene base polymer is a heterophasic propylene copolymer having a matrix of a propylene homopolymer and a dispersed phase of an elastomeric copolymer of propylene and at least one olefin comonomer; has a comonomer content of 2-7% by weight, based on the weight of the heterophasic propylene copolymer; has a melt flow rate MFR (2/230), determined according to ISO 1133 C4, of 0.1-2.0 g/10 min; has a broad molecular weight distribution as defined by its rheology shear thinning index, SHI 0/50 , measured at 200° C. of 9-30; has a tensile modulus, determined according to ISO 527-2/1B at 1 mm/min and 23° C. of at least 1800 MPa; has an impact strength, determined according to ISO 179/1 eA of at least 6 kJ/m 2 at 0° C. and at least 2 kJ/m 2 at −20° C. The composition is a polymer composition as defined above. The process is characterized by polymerizing in the presence of a stereospecific Ziegler-Natta catalyst including an electron donor:(i) a propylene homopolymer matrix in at
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A pressureless polymer pipe, wherein the polymer pipe comprises a propylene polymer composition comprising a propylene base polymer, wherein the propylene base polymer is a heterophasic propylene copolymer having a matrix of a multimodal propylene homopolymer, wherein the multimodal propylene homopolymer is produced in two or more reactors in series in the presence of different concentrations of hydrogen, and a dispersed phase of an elastomeric copolymer of propylene and at least one olefin comonomer; has a comonomer content of 2-7% by weight, based on the weight of the heterophasic propylene
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (15)
Non-Patent Literature (5)
- Chinese Office Action for corresponding Chinese Patent Application No. 200580029658.4 dated Apr. 19, 2010.
- Chinese Office Action for corresponding Chinese Patent Application No. 200580029658.4 dated Aug. 30, 2010.
- Czaja, K. et al. "Two-step polymerization of propylene over MgCl2-supported titanium catalyst", Macromol. Chem. Phys., vol. 199, 1998, pp. 451-455.
- Encyclopedia of Polymer Science and Engineering, Second Edition. vol. 6, Nov. 1986, p. 545-558.
- Heino et al. "Rheological Characterization of Polyehtylene Fractions." Theoretical and Applied Rheology. (1992), pp. 360-362).