Method of manufacturing and using rod-shaped proppants and anti-flowback additives
Abstract
A sintered rod-shaped proppant and anti-flowback agent possesses high strength and high conductivity. The sintered rods comprise between about 0.2% by weight and about 4% by weight aluminum titanate. In some embodiments, the sintered rods are made by mixing bauxitic and non-bauxitic sources of alumina that may also contain several so-called impurities (such as TiO 2 ), extruding the mixture, and sintering it. The starting material may optionally be milled to achieve better compacity and crush resistance in the final sintered rod. A fracturing fluid may comprise the sintered rods alone or in combination with a proppant, preferably a proppant of a different shape.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 9.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for making a proppant or antiflowback additive, the method comprising: mixing a ceramic precursor and at least one binding agent to form an extrudable mixture; extruding the extrudable mixture to form a plurality of extruded rods; reducing the length of the extruded rods by at least partially drying the rods in a manner that results in breakage of the extruded rods to form dried extruded rods of reduced length; and sintering the dried extruded rods of reduced length to obtain the proppant or antiflowback additive.
- Claim 2Depends on #1
The method of claim 1 , wherein the length of the extruded rods is not reduced by cutting.
- Claim 3Depends on #1
The method of claim 1 , further comprising fractionating the proppant or antiflowback additive to obtain a subset of rods having a desired range of lengths.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗