Patents
US 8,561,909 B2#43408517 Most CitedActiveUnited States (USPTO)Utility

RFID device having low-loss barium-based ceramic oxide

2Forward Citations (#43408517 Global)
0.1/yrCitation Velocity (#38984799 Global)
0.93Citation PageRank (#45933171 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An RFID chip is embedded in a device having a body that includes a low-dielectric loss material including at least one of barium stannate, barium cerate, barium tungstate and barium molybdate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method, comprising: providing a body material including at least one of barium stannate, barium cerate, barium tungstate and barium molybdate, said providing a body material including providing a precursor mixture that includes barium carbonate and tin oxide and heating the precursor mixture to form a ceramic oxide; and embedding a radio frequency identification (RFID) chip in the body material.

  2. Claim 2Depends on #1

    The method of claim 1 wherein providing a body material further includes mixing with the ceramic oxide a low-dielectric constant modifier including at least one of a magnesium aluminum silicate, a magnesium silicate, a zinc silicate, silica, and talc.

  3. Claim 3Depends on #2

    The method of claim 2 wherein providing a body material further includes sintering the mixture of ceramic oxide and low-dielectric constant modifier to pro

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗