A tube for a heat exchanger is formed by bending a three-layer clad material of an aluminum alloy to have an overlapped portion. The three-layer clad material is formed by a core material layer containing Mg not smaller than 0.2 wt % after brazing, a brazing material layer on one surface of the core material layer, and a high melting-point material layer on the other surface of the core material layer. The brazing material layer has a thickness not smaller than 25 μm before the brazing, and has a melting point lower than 600° C. The high melting-point material layer has a melting point equal to or higher than 600° C. In addition, the brazing material layer and the high melting-point material layer opposite to each other in the overlapped portion are bonded by the brazing at a temperature not lower than 450° C. for a time within 12 minutes.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 36 · Forward citations: 0.

Claims (9)

  1. Claim 1Independent Claim

    A tube for a heat exchanger, the tube being formed by bending a three-layer clad material of an aluminum alloy to have an overlapped portion bonded by brazing, the three-layer clad material comprising: a core material layer containing therein Mg equal to or larger than 0.2 wt % after the brazing; a brazing material layer provided on a first surface of the core material layer, wherein the brazing material layer has a thickness equal to or larger than 25 μm before the brazing, and has a melting point lower than 600° C.; and a high melting-point material layer provided on a second surface of the core material layer opposite the first surface, the high melting-point material layer having a melting point equal to or higher than 600° C., wherein the brazing material layer and the high melting-point material layer are in direct contact with each other in the overlapped portion, and are bonded to each other in the overlapped portion by the brazing at a brazing temperature not lower than 450° C. for a time within 12 minutes; and the overlapped portion includes a first high melting point material layer, a first core material layer, a first brazing material layer, a second high melting point material layer, a second core material layer and a second brazing material layer in this order from an inside of the tube to an outside of the tube.

  2. Claim 2Depends on #1

    The tube for a heat exchanger according to claim 1 , wherein the brazing temperature is in a temperature range equal to or higher than 450° C. and lower than 600° C.

  3. Claim 3Depends on #1

    The tube for a heat exchanger according to claim 1 , wherein the high melting-point material layer is a sacrifice material layer having a sacrifice anode effect with respect to the core material layer.

  4. Claim 4Depends on #1

    A heat exchanger for performing heat exchange, the heat exchange includes the tube according to claim 1 .

  5. Claim 5Depends on #1

    The tube for a heat exchanger according to claim 1 , wherein the tube defines an internal fluid passage, the high melting material layer being in direct contact with fluid in the internal fluid passage.

  6. Claim 6Depends on #1

    The tube for a heat exchanger according to claim 1 , wherein a first surface of the tube directly contacts a second surface of the tube opposite to the first surface in the overlapped portion.

  7. Claim 7Independent Claim

    A tube for a heat exchanger, the tube being formed by bending a three-layer clad material of an aluminum alloy to have an overlapped portion bonded by brazing, the three-layer clad material comprising: a core material layer containing therein Mg equal to or larger than 0.2 wt % after the brazing; a brazing material layer provided on a first surface of the core material layer, wherein the brazing material layer has a thickness equal to or larger than 25 μm before the brazing, and has a melting point lower than 600° C.; and a high melting-point material layer provided on a second surface of the core material layer opposite the first surface, the high melting-point material layer having a meltinq point equal to or higher than 600° C., wherein the brazing material layer and the high melting-point material layer are in direct contact with each other in the overlapped portion, and are bonded to each other in the overlapped portion by the brazing at a brazing temperature not lower than 450° C. for a time within 12 minutes; and first non-linear end of the tube overlaps a second non-linear end of the tube to form the overlapped portion.

  8. Claim 8Depends on #7

    The tube for a heat exchanger according to claim 7 , wherein the brazing temperature is in a temperature range equal to or higher than 450° C. and lower than 600° C.

  9. Claim 9Depends on #7

    The tube for a heat exchanger according to claim 7 , wherein the high melting-point material layer is a sacrifice material layer having a sacrifice anode effect with respect to the core material layer.

Technical Overview & Description

CROSS REFERENCE TO RELATED APPLICATION This application is based on Japanese Patent Application No. 2009-092390 filed on Apr. 6, 2009, the contents of which are incorporated herein by reference in its entirety. FIELD OF THE INVENTION The present invention relates to a tube and a heat exchanger using the tube, and a method of manufacturing the tube. The tube is made of a three-layer clad material of an aluminum alloy. BACKGROUND OF THE INVENTION Conventionally, a heat exchanger is made of a three-layer clad material of an aluminum alloy, including a brazing material layer, a core material layer and a sacrifice material layer. In the heat exchanger, a flat tube is formed by bending the three-layer clad material. Component parts of the heat exchanger including a plurality of the tubes are assembled, and then the components parts are brazed by heating, so as to form the heat exchanger. Recently, it is necessary to reduce the thickness of the component parts in order to reduce the entire weight of the heat exchanger. With this, in order to reduce the thickness of the component parts while the mechanical strength and the durability of the heat exchanger are maintained, the material for forming the tube is required to have a high strength. For example, JP 2006-131923A describes regarding an aluminum alloy clad material in which magnesium (Mg) is added in a core material layer in order to increase the strength. However, when Mg is added in the core material layer, the Mg in the core material layer diffuses to the surface of the brazing material layer, and reacts with flux in a brazing, thereby forming a high melting-point chemical composition such as MgF2. Thus, the flux component is reduced in the brazing, thereby reducing the brazing performance. In the clad material of the aluminum alloy described in JP 2006-131923A, a middle material layer is formed between the core material layer and the brazing material layer, so as to r

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (36)

PatentTitleYearCitations

Non-Patent Literature (5)

  • Examination Report dated Feb. 5, 2013 in corresponding Chinese Application No. 2010 1015 6855.5 with English translation.
  • Office Action dated Jul. 2, 2012 in corresponding Chinese Application No. 2010-10156855.5 with English translation.
  • Office action dated Nov. 30, 2011 in corresponding Chinese Application No. 2010 10156855.5.
  • Office Action dated Oct. 2, 2012 issued in corresponding Japanese Application No. 2009-092390 with English translation.
  • Office Action mailed May 28, 2013 in the corresponding JP Application No. 2009-092390 with English translation thereof.