High intrinsic viscosity melt phase polyester polymers with acceptable acetaldehyde generation rates
Abstract
A method for the production of solid polyester polymer particles comprising: a) polycondensing a molten polyester polymer composition in the presence of a polycondensation catalyst composition comprising antimony species; b) continuing the polycondensation of the molten polyester polymer composition to an It.V. of 0.68 dL/g or more; and c) after reaching an It.V. of 0.68 dL/g or more, adding a catalyst stabilizer or deactivator to the polymer melt; and d) after reaching an It.V. of 0.68 dL/g or more, solidifying the melt into solid polyester polymer particles which do not contain organic acetaldehyde scavengers. In a further embodiment, after solidification of the polyester from the melt phase polycondensation process: e) the amount of residual acetaldehyde in the particles in the solid state is reduced to a level of 10 ppm or less without increasing the It.V. of the particles by more than 0.03 dL/g. Such particles having an AA (acetaldehyde) generation rate of 20 ppm or less upon being melted after solidification following the melt phase production and a free AA level reduced after melt phase production to 10 ppm or less are introduced into a melt processing zone to make articles
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for the production of solid polyester polymer particles comprising: (a) polycondensing a molten polyester polymer composition in the presence of at least one polycondensation catalyst composition comprising antimony species; (b) continuing the polycondensation of the molten polyester polymer composition to an intrinsic viscosity (It.V.) of 0.68 dL/g or more; (c) after reaching an intrinsic viscosity (It.V.) of 0.68 dL/g or more, adding at least one antimony catalyst stabilizer or deactivator to the polymer melt; and (d) after reaching an intrinsic viscosity (It.V.) of 0.68 dL/g or mor
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 10,792,596 B1 | Pipeline filter | 2020 | 8 |
| US 11,014,027 B1 | Pipeline filter | 2021 | 4 |
| US 12,102,946 B1 | Pipeline filter | 2024 | 0 |
| US 11,154,801 B1 | Pipeline filter | 2021 | 2 |
| US 11,311,828 B1 | Pipeline filter | 2022 | 2 |
| US D903063 S | Filter housing | 2020 | 9 |