Patents
US 8,557,905 B2#34035445 Most CitedActiveUnited States (USPTO)Utility

Heat-dissipating resin composition used for LED light housing and heat-dissipating housing for LED lighting

3Forward Citations (#34035445 Global)
0.2/yrCitation Velocity (#31069733 Global)
0.96Citation PageRank (#44390377 Global)
11Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Provided is a novel heat-dissipating resin composition used for an LED light housing, the composition having excellent heat dissipation, fire retardancy, insulation properties, and molding processability as well as low specific gravity and improved whiteness. Also provided is a heat-dissipating housing for LED lighting, the housing being molded using the heat-dissipating resin composition. Disclosed is a heat-dissipating resin composition used for an LED light housing, comprising: 100 parts by mass of a thermoplastic resin composition (X) comprising 40 to 65% by mass of a polyamide resin (A), 33.5 to 59.8% by mass of a metal-hydroxide-based fire retardant (B), and 0.2 to 1.5% by mass of a polytetrafluoroethylene resin (C); and 5 to 200 parts by mass of an inorganic filler (Y) comprising 5 to 100% by mass of boron nitride (D) and 0 to 95% by mass of an inorganic oxide filler (E), wherein thermal conductivity is equal to or greater than 1.0 W/m·K. Also, disclosed is a heat-dissipating housing for LED lighting, the housing being molded using the heat-dissipating resin composition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 3.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A heat-dissipating resin composition used for an LED light housing, comprising: 100 parts by mass of a thermoplastic resin composition (X) comprising 40 to 65% by mass of a polyamide resin (A), 33.5 to 59.8% by mass of a metal-hydroxide-based fire retardant (B), and 0.2 to 1.5% by mass of a polytetrafluoroethylene resin (C); and 5 to 200 parts by mass of an inorganic filler (Y) comprising 5 to 100% by mass of boron nitride (D) and 0 to 95% by mass of an inorganic oxide filler (E), wherein a thermal conductivity of the composition is equal to or greater than 1.0 W/m·K.

  2. Claim 2Depends on #1

    The heat-dissipating resin composition according to claim 1 , wherein the boron nitride (D) has a volume-average particle diameter of from 5 to 25 μm as determined by a laser diffraction and scattering method.

  3. Claim 3Independent Claim

    The heat-dissipati

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • International Search Report; Application No. PCT/JP2011/057366; Form PCT/ISA/2010 (4 pages).