Reinforced flame retardant resin composition and molded article
Abstract
A reinforced flame retardant resin composition including 20 to 87% by mass of an (A) thermoplastic resin, 3 to 20% by mass of a (B) aromatic phosphoric acid ester-based flame retardant agent, 5 to 40% by mass of (C) mica powder, and 0.5 to 30% by mass of (D) hydrous mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 2.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A reinforced flame retardant resin composition comprising: 20 to 87% by mass of an (A) thermoplastic resin; 3 to 20% by mass of a (B) aromatic phosphoric acid ester-based flame retardant agent; 5 to 40% by mass of (C) mica powder; and 0.5 to 30% by mass of (D) chlorite group mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C.
- Claim 2Depends on #1
The reinforced flame retardant resin composition according to claim 1 comprising: 30 to 87% by mass of the (A) component; 3 to 20% by mass of the (B) component; 5 to 30% by mass of the (C) component; and 0.5 to 20% by mass of the (D) component, wherein a total amount of the (C) component and the (D) component is 10 to 50% by mass.
- Claim 3Depends on #1
The reinforced flame retardant resin composition according to claim 1 fu
Technical Overview & Description