Reducing dross method of lead-free solder

1Forward Citations (#60807195 Global)
0.1/yrCitation Velocity (#49595372 Global)
0.76Citation PageRank (#60807195 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A reducing dross method of lead-free solder includes the steps of: producing master alloy of reducing dross which comprises Sn and 0.1 to 0.8 wt % P; analyzing the percentage of P of the lead-free solder to be modified, in order to reach 0.008 to 0.015 wt % P in the lead-free solder, adding the master alloy into the lead-free solder with the percentage of P less than 0.008 wt % or no P; then sampling the lead-free solder at regular intervals to determine the percentage and the percentage loss of P, if the percentage of P being less than a given value from 0.008 to 0.015 wt %, adding the master alloy to keep the percentage of P as 0.008 to 0.015 wt %.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A reducing dross method of lead-free solder, comprising the steps of: firstly producing alloy of reducing dross by a master alloy process, the alloy of reducing dross comprising Sn and 0.1 to 0.8 wt % P; analyzing a percentage of P of the lead-free solder to be modified in a soldering furnace; if the percentage of P of the lead-free solder is less than 0.008 wt %, adding the alloy of reducing dross into the lead-free solder until the percentage of P of the lead-free solder in the soldering furnace reaches within 0.008 to 0.015 wt % P; then sampling the lead-free solder in the soldering furnace