Abstract
A nonvolatile memory device and methods of manufacturing the same has one electrode with a higher work function and a second electrode with a lower work function. The nonvolatile memory device further comprises one or more resistive random access memory (RRAM) cells. The RRAM cells comprise a semiconductor layer with a bandgap of at least four electron volts and a barrier layer between the semiconductor layer and one of the electrodes.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of fabricating a memory cell, the method comprising: forming a first electrode, the first electrode comprising a first material comprising a first element, the first electrode disposed atop a substrate; forming a semiconductor layer, the semiconductor layer disposed over the first electrode, the semiconductor layer comprising a second material having a bandgap of at least four electron volts; forming a second electrode, the second electrode disposed over the semiconductor layer, the second electrode and the first electrode having different work functions; forming a dielectric barrier
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 15 total)
References Cited — Backward Prior Art (14)
Non-Patent Literature (3)
- MJ Sanchez et al, "A mechanism for unipolar resistance switching in oxide nonvolatile memory devices," Applied Physics Letters 91, 252101, 2007, American Institute of Physics.
- Pang Shiu Chen et al., "HfOx Thin Films for Resistive Memory Device by Use of Atomic Layer Deposition," Mater. Res. Soc. Symp. Proc. vol. 997 © 2007 Materials Research Society.
- Seong Keun Kim et al., "High dielectric constant TiO2 thin films on a Ru electrode grown at 250° C.by atomic-layer deposition," Applied Physics Letters, V.85, N.18, Nov. 1, 2004.